Material Notes:
Relene M60075 is a High Density Polyethylene grade suitable for injection molding applications where good mechanical properties, gloss, dimensional stability, and good ESCR are required. This grade is recommended for technical moldings like crates, luggage shells, helmets, defense applications etc.Information provided by Reliance Industries
Physical Properties Metric English Comments
Density 0.960 g/cc
0.0347 lb/in³
ASTM D1505
Melt Flow 8.2 g/10 min

@Load 2.16 kg
8.2 g/10 min

@Load 4.76 lb
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Shore D 69
69
ASTM D2240
Tensile Strength, Yield 25.0 MPa
3630 psi
ASTM D638
Elongation at Break 800 %
800 %
ASTM D638
Flexural Yield Strength 30.0 MPa
4350 psi
ASTM D790
Flexural Modulus 0.900 GPa
131 ksi
ASTM D790
Izod Impact, Notched 0.880 J/cm
1.65 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Vicat Softening Point 128 °C
262 °F
ASTM D1525
Processing Properties Metric English Comments
Processing Temperature 220 - 250 °C
428 - 482 °F
Recommended injection moulding temperature