Material Notes:
Key PropertiesExcellent adhesion to low surface energy plastics without primer or surface preparation.ApplicationsHigh flexibility, 200% elongation, emphasizing high tack for un-abraded substrates and poorly prepared surfaces. Excellent water and oil sealing. Ambient or thermal cure. May be catalyzed for fast set time.Information provided by Reltek LLC
Physical Properties Metric English Comments
Specific Gravity 1.05 g/cc
1.05 g/cc
A
1.42 g/cc
1.42 g/cc
B