Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Renegade Materials Corporation RM-3002 Bismaleimide (BMI) Resin 4581 Astroquartz III

Category Polymer , Thermoset , Filled/Reinforced Thermoset
Manufacturer Renegade Materials Corporation
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Renegade Materials Corporation RM-3002 Bismaleimide (BMI) Resin 4581 Astroquartz III.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Developed using state-of-the-art formulating technologies, RM-3002 BMI prepreg products deliver superior hot/wet performance in airframe, missile and propulsion applications at service temperatures up to 400°F. RM-3002 “next-generation” BMI delivers improved damage tolerance at higher temperatures vs. industry-standard BMI’s. Renegade precision-quality prepregs exhibit excellent handling characteristics and are available in woven and unidirectional form on various fibers including carbon, quartz and S2 glass. A wide variety of nano-materials can be incorporated into this resin system for tailored laminate properties and multi-functional performance. Renegade offers paste (RM-3006 and RM-3007) and film (RM-3011) adhesives compatible with RM-3002. Renegade also offers similar resin systems for RTM (RM-3000) or VARTM (RM-3010) processing.Information provided by Renegade Materials Corporation.
Physical Properties Metric English Comments
Density 1.26 g/cc
0.0456 lb/in³
Resin
Mechanical Properties Metric English Comments
Elongation at Break 3.6 %
3.6 %
Resin
Flexural Strength 145 MPa
21000 psi
Resin
Flexural Modulus 4.27 GPa
620 ksi
Resin
Compressive Strength 538 MPa
78000 psi
Combined Loading Compression, Dry, RT; ASTM D6641-09
Compressive Modulus 26.2 GPa
3800 ksi
Combined Loading Compression, Dry, RT; ASTM D6641-09
Shear Strength 89.6 MPa
13000 psi
Notched Compression In-plane, Dry, RT; ASTM D3846-02
Electrical Properties Metric English Comments
Dielectric Constant 3.3

@Frequency 1.00e+10 Hz
3.3

@Frequency 1.00e+10 Hz
X-band; ASTM D2520
Dissipation Factor 0.0050

@Frequency 1.00e+10 Hz
0.0050

@Frequency 1.00e+10 Hz
X-band