Resin Technology Group DP031199-1 Cationic UV Cure Epoxy Adhesive

Category Polymer , Adhesive , Thermoset , Epoxy , Epoxy Adhesive
Manufacturer Resin Technology Group
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Resin Technology Group DP031199-1 Cationic UV Cure Epoxy Adhesive.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
DP031199-1 is an epoxy-based, low-viscosity, cationic-curable adhesive/sealant. This product is activated by exposure to medium intensity UV radiation resulting in a strong, chemically resistant, low out-gassing polymer system. This UV curable adhesive is soft and flexible and cures tack free.Developmental Product: This data was generated on laboratory material and should not be used for specification purposes. The Developmental Product name and designation may change upon commercialization.Processing: UV light cure: Intensity of 200 mw/cm2; Spectral output of 300 to 500 nanometers; Optimum wavelength of 375 nanometersRecommended Aurora UV light sources:Aurora 455-S 5x5 High Intensity FloodAurora 461-S 1x6 High Intensity BeamAurora 100-S Spot Light GuideInformation provided by Resin Technology Group.
Physical Properties Metric English Comments
Specific Gravity 1.07 g/cc
1.07 g/cc
Uncured
Viscosity 1500 cP

@Temperature 25.0 °C
1500 cP

@Temperature 77.0 °F
Uncured
Mechanical Properties Metric English Comments
Hardness, Shore A 50
50
Cured
Elongation at Break 8.0 %
8.0 %
Cured
Shear Strength 41.4 MPa
6000 psi
Cured, tensile
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 160 °C
320 °F
Cured
Minimum Service Temperature, Air -50.0 °C
-58.0 °F
Cured
Flash Point >= 93.3 °C
>= 200 °F
Uncured
Optical Properties Metric English Comments
Transmission, Visible 80 %
80 %
Mfr. Specifies clear but does not quantify
Descriptive Properties Value Comments
Color Clear
Composition Epoxy
Moisture Resistance Excellent
Cured