Resin Technology Group Fusion 508 Industrial Grade Gel Fusion Cyanoacrylate

Category Polymer , Adhesive , Thermoset , Acrylic/Cyanoacrylate Adhesive
Manufacturer Resin Technology Group
Trade Name Fusion
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Resin Technology Group Fusion 508 Industrial Grade Gel Fusion Cyanoacrylate.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by Resin Technology Group.
Mechanical Properties Metric English Comments
Shear Strength 26.0 MPa
3770 psi
Tensile
Optical Properties Metric English Comments
Transmission, Visible 80 %
80 %
Mfr. Specifies clear but does not quantify
Descriptive Properties Value Comments
Base Ethyl
Color Clear
Viscosity Gel