Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Resin Technology Group TIGA 110-EXDP Low Viscosity, Optically Clear Glass Bonder

Category Polymer , Adhesive , Thermoset , Epoxy , Epoxy Adhesive
Manufacturer Resin Technology Group
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Resin Technology Group TIGA 110-EXDP Low Viscosity, Optically Clear Glass Bonder.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Mix ratio 100/50 by volume.TIGA 110EX-DP is a transparent, low viscosity epoxy resin formulation recommended for industrial adhesive, small potting and laminating applications where sparkling clarity and excellent structural, mechanical and electrical properties are required. This two-part adhesive exhibits good wetting, cures at room temperature and develops strong, low shrinkage, bonds to most materials including optical fibers, glass, ceramics, most metals and many rigid plastics. It has excellent dimensional stability over a wide temperature range. Fully cured TIGA 110EX-DP is a durable electrical insulator with good physical properties, plus resistance to water, weather, ozone and oxygen, petroleum solvents, lubricating oils, jet fuel, gasoline, alcohol, salt solutions, mild acids and alkalis and many other organic and inorganic compounds.Information provided by Resin Technology Group.
Physical Properties Metric English Comments
Specific Gravity 1.15 g/cc
1.15 g/cc
Viscosity 2500 cP

@Temperature 25.0 °C
2500 cP

@Temperature 77.0 °F
Mixed
Collected Volatile Condensable Material 0.010 %
0.010 %
2 hours at 100°C
Mechanical Properties Metric English Comments
Hardness, Shore D 83
83
Tensile Strength at Break >= 50.3 MPa
>= 7300 psi
Shear Strength 3.45 MPa

@Temperature 100 °C
500 psi

@Temperature 212 °F
Tensile lap
17.2 MPa

@Temperature 25.0 °C
2500 psi

@Temperature 77.0 °F
Tensile lap
Thermal Properties Metric English Comments
CTE, linear 54.0 µm/m-°C

@Temperature 20.0 °C
30.0 µin/in-°F

@Temperature 68.0 °F
Maximum Service Temperature, Air 135 °C
275 °F
Softening Point 75.0 °C
167 °F
Minimum Service Temperature, Air -60.0 °C
-76.0 °F
Glass Transition Temp, Tg 60.0 °C
140 °F
Optical Properties Metric English Comments
Refractive Index 1.58
1.58
Transmission, Visible 80 %
80 %
Mfr. Specifies clear but does not quantify
Electrical Properties Metric English Comments
Dielectric Strength >= 15.7 kV/mm
>= 400 kV/in
Processing Properties Metric English Comments
Cure Time 30.0 min

@Temperature 65.0 °C
0.500 hour

@Temperature 149 °F
1440 min

@Temperature 25.0 °C
24.0 hour

@Temperature 77.0 °F
Pot Life 30 min
30 min
Small Mass
Descriptive Properties Value Comments
Color Clear
Users viewing this material also viewed the following: