Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Resin Technology Group TIGA 901 Room Temperature Curing Silver Conductive Epoxy

Category Polymer , Adhesive , Thermoset , Epoxy , Epoxy Adhesive , Epoxy, Electrically Conductive
Manufacturer Resin Technology Group
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Resin Technology Group TIGA 901 Room Temperature Curing Silver Conductive Epoxy.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
100 parts resin to 6 parts hardener. Cure 24 hours at 25°C, 1-4 hours at 65°C, 30-60 minutes at 125°C, or 30 minutes at 150°C.TIGA 901 is an electrically conductive, silver filled epoxy adhesive recommended for electronic bonding and sealing applications that require a combination of good mechanical and electrical properties. This two-part smooth paste formulation of refined pure silver and epoxy is free of solvents and copper or carbon additives. It develops strong, durable, electrically and thermally conducting bonds and coatings between many different and dissimilar materials such as metals, ceramics, glass and plastic laminates. TIGA 901 cures at room temperature and can be used as a “cold-solder” for heat sensitive components where hot soldering is impractical.Applications: This product can be used for the assembly and repair of electrical modules, printed circuits, wave guides, flat cable and high frequency shields.Information provided by Resin Technology Group.
Physical Properties Metric English Comments
Specific Gravity 2.50 g/cc
2.50 g/cc
Solids Content 100 %
100 %
Mechanical Properties Metric English Comments
Hardness, Shore D 85
85
Shear Strength 6.89 MPa
1000 psi
Cured 1 hour at 65°C, Alum/Alum
13.1 MPa
1900 psi
Cured 60 minutes at 125°C, Alum/Alum
Thermal Properties Metric English Comments
CTE, linear 25.0 µm/m-°C

@Temperature 20.0 °C
13.9 µin/in-°F

@Temperature 68.0 °F
Thermal Conductivity 6.05 W/m-K
42.0 BTU-in/hr-ft²-°F
Maximum Service Temperature, Air 125 °C
257 °F
Minimum Service Temperature, Air -60.0 °C
-76.0 °F
Electrical Properties Metric English Comments
Volume Resistivity 0.00030 ohm-cm
0.00030 ohm-cm
cured 60 minutes at 125°C
0.0090 ohm-cm
0.0090 ohm-cm
cured 1 hour at 65°C
Processing Properties Metric English Comments
Cure Time 30.0 min

@Temperature 250 °C
0.500 hour

@Temperature 482 °F
30.0 - 60.0 min

@Temperature 125 °C
0.500 - 1.00 hour

@Temperature 257 °F
60.0 - 240 min

@Temperature 65.0 °C
1.00 - 4.00 hour

@Temperature 149 °F
1440 min

@Temperature 25.0 °C
24.0 hour

@Temperature 77.0 °F
Pot Life 90.0 min

@Temperature 25.0 °C
90.0 min

@Temperature 77.0 °F
20 gm mass
Descriptive Properties Value Comments
Color Silver
Outgassing Low
Viscosity Smooth paste
After mixing
Copyright © lookpolymers.com All Rights Reserved