Material Notes:
Resinlab™ AR 4340 HP is a 1:1 mix methacrylate-based structural adhesive designed for general purpose bonding of a wide variety of materials in industrial applications. It is an accelerated version of AR 4305. AR 4340 HP forms tough, durable bonds to most plastics, composites, metals, ceramics, and woods in all combinations. Surface cleaning or preparation, or the use of primers, or chemical wipes is not required in almost all cases. AR 4340 HP is a very fast curing product with gelling of the mixed adhesive within 2-3 minutes and fixture in 3-5 minutes at room temperature. The cure time was designed for high speed manufacturing processes where fast fixturing is required. AR 4340 HP is easily dispensed from packaged cartridges or with commercial dispensing equipment as a non-sag, creamy gel, with no stringing. The product was designed to be used with static mixer tubes and has a balanced viscosity between parts. There are no abrasive fillers or extenders to reduce performance or cause wear in dispensing equipment.Information Provided by Resinlab L.L.C., an Ellsworth Adhesives Company.
Physical Properties Metric English Comments
Viscosity 80000 cP
80000 cP
Part B, Spindle TD, 2.5 rpm; Uncured
90000 cP
90000 cP
Part A, Spindle TD, 2.5 rpm; Uncured
250000 cP
250000 cP
Spindle TD, 2.5 rpm; Curing
Mechanical Properties Metric English Comments
Hardness, Shore D 60
60
Cured
Elongation at Yield 70 %
70 %
Cured
Adhesive Bond Strength 17.9 MPa
2600 psi
alum/aluminum
24.1 MPa
3500 psi
steel/steel
Impact >= 11
>= 11
[J/in^2]; FRP/FRP; auto side impact
Peel Strength >= 5.26 kN/m
>= 30.0 pli
steel/steel
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 121 °C
250 °F
Cured
Minimum Service Temperature, Air -40.0 °C
-40.0 °F
Flash Point 10.6 °C
51.0 °F
LCC; Uncured
Descriptive Properties Value Comments
Color Amber
Part B; Uncured
Natural
Part A; Uncured
Fixture Time (minutes) 3-4
Curing
Mix Ratio 1:1
Weight and Volume; Uncured
Working Time (minutes) 1
Curing