Resirene Resirene® 6220 High Impact Polystyrene

Category Polymer , Thermoplastic , Polystyrene (PS) , Polystyrene, Impact Modified
Manufacturer Resirene S.A. de C.V.
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Resirene Resirene® 6220 High Impact Polystyrene.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Features:Low FlowEasy ProcessingGood GlossHigh ElongationFDA Rating: 21 CFR 177.1640Mechanical StrengthApplications:Extrusion/ ThermoformingDisposablesGPPS/HIPS BlendsRefrigerator PartsInformation provided by US distributor Calsak Corporation.
Physical Properties Metric English Comments
Specific Gravity 1.04 g/cc
1.04 g/cc
ASTM D792
Linear Mold Shrinkage 0.0030 - 0.0070 cm/cm
0.0030 - 0.0070 in/in
ASTM D955
Melt Flow 3.8 g/10 min

@Load 5.00 kg,
Temperature 200 °C
3.8 g/10 min

@Load 11.0 lb,
Temperature 392 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength at Break 21.4 MPa
3100 psi
ASTM D638
Tensile Strength, Yield 22.8 MPa
3310 psi
ASTM D638
Elongation at Break 60 %
60 %
ASTM D638
Tensile Modulus 1.931 GPa
280.1 ksi
ASTM D638
Izod Impact, Notched 0.910 J/cm
1.70 ft-lb/in
0.5 in.; ASTM D256
1.07 J/cm
2.00 ft-lb/in
0.125 in.; ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 78.0 °C
172 °F
ASTM D648
Flammability, UL94 HB
HB