Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Rochling Engineered Plastics Polystone® G HDPE Extruded Sheet

Category Polymer , Thermoplastic , Polyethylene (PE) , HDPE , High Density Polyethylene (HDPE), Extruded
Manufacturer Rochling Engineered Plastics
Trade Name Polystone®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Rochling Engineered Plastics Polystone® G HDPE Extruded Sheet.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by Röchling Engineered Plastics.
Physical Properties Metric English Comments
Density 0.950 g/cc
0.0343 lb/in³
ASTM D792
Water Absorption <= 0.10 %
<= 0.10 %
ASTM D570
Mechanical Properties Metric English Comments
Hardness, Shore D 67
67
ASTM D785
Tensile Strength, Yield 20.7 MPa
3000 psi
ASTM D638
Flexural Modulus 0.793 GPa
115 ksi
ASTM D790
Izod Impact, Notched 1.66 J/cm
3.10 ft-lb/in
@ 73°F; ASTM D256
Thermal Properties Metric English Comments
CTE, linear 198 µm/m-°C

@Temperature 20.0 °C
110 µin/in-°F

@Temperature 68.0 °F
ASTM D696
Deflection Temperature at 0.46 MPa (66 psi) 79.4 °C
175 °F
ASTM D648