Rogers Corporation Bisco® L3 Premiere Next Generation Dynamic Flooring Material

Category Polymer , Thermoset , Silicone , Silicone Foam
Manufacturer Rogers Corporation
Trade Name Bisco®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Rogers Corporation Bisco® L3 Premiere Next Generation Dynamic Flooring Material.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
BISCO® L3 Premiere silicone foam technology is the next generation in dynamic and floating floor materials from Rogers Corporation developed specifically to meet the most challenging global requirements for flammability, smoke and toxicity.The L3 Premiere exhibits a low natural frequency and is engineered to isolate vibration enabling a safe and smooth passenger ride over the life-time of mass transit vehicles.Railcar dynamic and floating floor padsBoat and yacht flooring isolation padsInformation provided by Rogers Corporation.
Physical Properties Metric English Comments
Density 0.304 g/cc
0.0110 lb/in³
ASTM D1056
Water Absorption <= 5.0 %

@Time 86400 sec
<= 5.0 %

@Time 24.0 hour
Mechanical Properties Metric English Comments
Tensile Strength 0.345 MPa
50.0 psi
ASTM D142
Elongation at Break 50 %
50 %
ASTM D412
Compressive Yield Strength 0.110 MPa

@Strain 25.0 %
16.0 psi

@Strain 25.0 %
ASTM D1056
Compression Set <= 5.0 %

@Temperature 100 °C,
Time 79200 sec
<= 5.0 %

@Temperature 212 °F,
Time 22.0 hour
ASTM D1056
Descriptive Properties Value Comments
Mechanical Loss Factor 0.2
DMA
Stiffness Factor 1.5