Rostone Rosite® C200BS ESD SMC, Conductive Thermoset Polyester, 10% Glass Reinforced  (discontinued **)

Category Polymer , Thermoset , Composite SMC , Filled/Reinforced Thermoset , Polyester, TS , Thermoset Polyester Glass SMC
Manufacturer
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Rostone Rosite® C200BS ESD SMC, Conductive Thermoset Polyester, 10% Glass Reinforced  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Key Features: Electrostatic DissipativeRosite Conductive C used in applications such as molded paper guides in printers and plotters. Conductive C is the UL recognition.Information provided by Oneida-Rostone Group.
Physical Properties Metric English Comments
Density 1.60 g/cc
0.0578 lb/in³
ASTM D792
Water Absorption 0.33 %
0.33 %
24 hrs; ASTM D570
Linear Mold Shrinkage 0.0010 cm/cm
0.0010 in/in
shrinkage
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 37.2 MPa
5400 psi
ASTM D638
Flexural Strength 145 MPa
21000 psi
ASTM D790
Flexural Modulus 8.30 GPa
1200 ksi
ASTM D790
Izod Impact, Notched 8.50 J/cm
15.9 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Flammability, UL94 5VA
5VA
0.062 inch thickness (pending)