Rotuba H Cellulose Acetate

Category Polymer , Renewable/Recycled Polymer , Thermoplastic , Cellulosic , Cellulose Acetate, Molded
Manufacturer Rotuba
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Rotuba H Cellulose Acetate.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Property values at 50% RH.Data provided by the manufacturer.
Physical Properties Metric English Comments
Density 1.28 g/cc
0.0462 lb/in³
ASTM D792
Water Absorption 2.3 %
2.3 %
ASTM D570
Mechanical Properties Metric English Comments
Hardness, Rockwell R 76
76
ASTM D785
Tensile Strength, Ultimate 40.0 MPa
5800 psi
ASTM D638
Tensile Strength, Yield 30.0 MPa
4350 psi
ASTM D638
Elongation at Break 39 %
39 %
ASTM D638
Flexural Yield Strength 46.0 MPa
6670 psi
ASTM D790
Flexural Modulus 0.120 GPa
17.4 ksi
ASTM D790
Izod Impact, Notched 2.08 J/cm
3.90 ft-lb/in
ASTM D256
0.590 J/cm

@Temperature -40.0 °C
1.11 ft-lb/in

@Temperature -40.0 °F
ASTM D256
Thermal Properties Metric English Comments
Melting Point 155 °C
311 °F
Flow temperature, ASTM D569
Processing Properties Metric English Comments
Processing Temperature 210 °C
410 °F
Center barrel temperature