Material Notes:
Product Description: BM1052 grade is a high molecular weight High Density Polyethylene copolymer with broad molecular weight distribution. It has excellent processability and exhibits very high impact strength, stiffness and superior environmental stress crack resistance.Typical Applications: BM1052 resin is intended for blow molding of large containers such as closed head shipping containers, fuel tanks and containers for industrial use. It can also be extruded into sheets giving exceptionally high impact strength.Information provided by SABIC.
Physical Properties Metric English Comments
Density 0.952 g/cc
0.0344 lb/in³
ASTM D1505
ESCR 100% Igepal® >= 1200 hour
>= 1200 hour
F50; ASTM D1693B
ESCR 10% Igepal® 720 hour
720 hour
F50; ASTM D1693B
Melt Flow 0.050 g/10 min

@Load 2.16 kg,
Temperature 190 °C
0.050 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
0.38 g/10 min

@Load 5.00 kg,
Temperature 190 °C
0.38 g/10 min

@Load 11.0 lb,
Temperature 374 °F
ASTM D1238
10 g/10 min

@Load 21.6 kg,
Temperature 190 °C
10 g/10 min

@Load 47.6 lb,
Temperature 374 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Shore D 63
63
ASTM D2240
Tensile Strength at Break 18.0 MPa
2610 psi
ASTM D638
Tensile Strength, Yield 27.0 MPa
3920 psi
ASTM D638
Elongation at Break >= 500 %
>= 500 %
ASTM D638
Flexural Strength 26.0 MPa
3770 psi
ASTM D790
Flexural Modulus 1.05 GPa
152 ksi
ASTM D790
1% Secant Modulus >= 1000 MPa
>= 145000 psi
ASTM D638
Izod Impact, Notched 3.00 J/cm
5.62 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Vicat Softening Point 125 °C
257 °F
ASTM D1525
Brittleness Temperature <= -75.0 °C
<= -103 °F
ASTM D746
Processing Properties Metric English Comments
Melt Temperature 200 - 230 °C
392 - 446 °F