Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

SABIC HC 050 Amorphous Polyethylene Terephthalate

Category Polymer , Thermoplastic , Polyester, TP , Polyethylene Terephthalate (PET) , Polyethylene Terephthalate (PET), Unreinforced
Manufacturer SABIC
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF SABIC HC 050 Amorphous Polyethylene Terephthalate.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Product Description: HC 050 is an amorphous, low molecular weight thermoplastic PET made by a continuous melt-phase polymerization process.Characteristics: HC 050 is a specially formulated amorphous PET grade.Typical Applications: HC 050 is especially suitable for filament, fiber spinning and film applications. It can also be used as an intermediate for solid state polymerization to make PET with high I.V.Information provided by SABIC.
Physical Properties Metric English Comments
Density 1.333 g/cc
0.04816 lb/in³
crystalline density; SABIC (IRC0032)
Viscosity Test 62 - 66 cm³/g
62 - 66 cm³/g
Intrinsic; SABIC (IRC0041)
Maximum Moisture Content <= 0.40
<= 0.40
% w/w; SABIC (IRC0050)
Thermal Properties Metric English Comments
Melting Point 240 - 260 °C
464 - 500 °F
SABIC (IRC0053)
Descriptive Properties Value Comments
Color (b) -5.0 ± 1.0
Color (L) 82 ± 2
DEG Content = 1.2 % w/w
SABIC (IRC0055)
Dust Content < 0.01 % w/w
SABIC (IRC0060)