Category Polymer , Thermoplastic , ABS Polymer , Polycarbonate/ABS Alloy, Unreinforced , Polycarbonate (PC)
Manufacturer SABIC Innovative Plastics (GE Plastics)
Trade Name Cycoloy®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF SABIC Innovative Plastics Cycoloy® CY201 PC+ABS (Europe-Africa-Middle East).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Cycoloy* CY201 is an industrial quality PC+ABS Flame Retardant grade for injection moulding applications.
Physical Properties Metric English Comments
Density 1.19 g/cc
0.0430 lb/in³
ISO 1183
Linear Mold Shrinkage, Flow 0.0040 - 0.0060 cm/cm
0.0040 - 0.0060 in/in
on Tensile Bar; SABIC Method
Melt Index of Compound 20 g/10 min

@Load 2.16 kg,
Temperature 260 °C
20 g/10 min

@Load 4.76 lb,
Temperature 500 °F
MVR [cm^3/10 min]; ISO 1133
Mechanical Properties Metric English Comments
Tensile Strength at Break 45.0 MPa
6530 psi
50 mm/min; ISO 527
Tensile Strength, Yield 60.0 MPa
8700 psi
50 mm/min; ISO 527
Elongation at Yield 3.0 %
3.0 %
50 mm/min; ISO 527
Tensile Modulus 2.50 GPa
363 ksi
1 mm/min; ISO 527
Flexural Yield Strength 85.0 MPa
12300 psi
2 mm/min; ISO 178
Flexural Modulus 2.50 GPa
363 ksi
2 mm/min; ISO 178
Izod Impact, Notched (ISO) 6.00 kJ/m²
2.86 ft-lb/in²
80*10*4; ISO 180/1A
4.00 kJ/m²

@Temperature -30.0 °C
1.90 ft-lb/in²

@Temperature -22.0 °F
80*10*4; ISO 180/1A
Charpy Impact, Notched 0.600 J/cm²
2.86 ft-lb/in²
Edgew 80*10*4 sp=62mm; ISO 179/1eA
0.400 J/cm²

@Temperature -30.0 °C
1.90 ft-lb/in²

@Temperature -22.0 °F
Edgew 80*10*4 sp=62mm; ISO 179/1eA
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 90.0 °C
194 °F
Edgew 120*10*4 sp=100mm; ISO 75/Be
Deflection Temperature at 1.8 MPa (264 psi) 80.0 °C
176 °F
Edgew 120*10*4 sp=100mm; ISO 75/Ae
Vicat Softening Point 95.0 °C
203 °F
Rate B/120; ISO 306
Flammability, UL94 V-1

@Thickness 1.50 mm
V-1

@Thickness 0.0591 in
UL 94
V-0

@Thickness 2.00 mm
V-0

@Thickness 0.0787 in
UL 94
Glow Wire Test 960 °C

@Thickness 3.20 mm
1760 °F

@Thickness 0.126 in
IEC 60695-2-12
Descriptive Properties Value Comments
Ball Pressure Test, 75°C +/- 2°C PASSES
IEC 60695-10-2