Category Polymer , Thermoplastic , ABS Polymer , Polycarbonate/ABS Alloy, Unreinforced , Polycarbonate (PC)
Manufacturer SABIC Innovative Plastics (GE Plastics)
Trade Name Cycoloy®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF SABIC Innovative Plastics Cycoloy® FXC810AR PC+ABS.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Color Package may affect performance. Visual Fx PC+ABS in various metallic (Ares) colors. High heat/good flow characteristics. Appliance/automotive/telecommunication uses.
Physical Properties Metric English Comments
Specific Gravity 1.18 g/cc
1.18 g/cc
ASTM D792
Linear Mold Shrinkage, Flow 0.0040 - 0.0060 cm/cm

@Thickness 3.20 mm
0.0040 - 0.0060 in/in

@Thickness 0.126 in
SABIC Method
Melt Flow 22 g/10 min

@Load 5.00 kg,
Temperature 260 °C
22 g/10 min

@Load 11.0 lb,
Temperature 500 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength at Break 44.0 MPa
6380 psi
Type I, 50 mm/min; ASTM D638
Tensile Strength, Yield 51.0 MPa
7400 psi
Type I, 50 mm/min; ASTM D638
Elongation at Break 50 %
50 %
Type I, 50 mm/min; ASTM D638
Elongation at Yield 5.0 %
5.0 %
Type I, 50 mm/min; ASTM D638
Tensile Modulus 2.48 GPa
360 ksi
50 mm/min; ASTM D638
Flexural Yield Strength 75.0 MPa
10900 psi
1.3 mm/min, 50 mm span; ASTM D790
Flexural Modulus 2.41 GPa
350 ksi
1.3 mm/min, 50 mm span; ASTM D790
Izod Impact, Notched 4.27 J/cm
8.00 ft-lb/in
ASTM D256
Dart Drop, Total Energy 40.0 J

@Temperature 23.0 °C
29.5 ft-lb

@Temperature 73.4 °F
ASTM D3763
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 72.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
40.0 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
CTE, linear, Transverse to Flow 72.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
40.0 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
Deflection Temperature at 0.46 MPa (66 psi) 131 °C

@Thickness 3.20 mm
268 °F

@Thickness 0.126 in
unannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 112 °C

@Thickness 3.20 mm
234 °F

@Thickness 0.126 in
unannealed; ASTM D648
Vicat Softening Point 143 °C
289 °F
Rate B/50; ASTM D1525