Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

SABIC Innovative Plastics Cycoloy® RCM6123 PC+ABS (Asia Pacific)

Category Polymer , Thermoplastic , ABS Polymer , Polycarbonate/ABS Alloy, Unreinforced , Polycarbonate (PC)
Manufacturer SABIC Innovative Plastics (GE Plastics)
Trade Name Cycoloy®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF SABIC Innovative Plastics Cycoloy® RCM6123 PC+ABS (Asia Pacific).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Cycoloy* RCM6123 resin is an injection moldable filled PC/ABS blend with non-brominated and non-chlorinated flame retardant. It contains 30% post consumer recycle content with a UL-94 V0 rating @ 1.2mm. Developed for thin wall applications that require high flow and high stiffness performance. Limited availability and restricted color only.
Physical Properties Metric English Comments
Specific Gravity 1.30 g/cc
1.30 g/cc
ASTM D792
Density 1.30 g/cc
0.0470 lb/in³
ISO 1183
Moisture Absorption 0.0400 %
0.0400 %
23°C / 50% RH; ISO 62
Linear Mold Shrinkage, Flow 0.0030 - 0.0040 cm/cm

@Thickness 3.20 mm
0.0030 - 0.0040 in/in

@Thickness 0.126 in
SABIC Method
Melt Flow 11 g/10 min

@Load 2.16 kg,
Temperature 260 °C
11 g/10 min

@Load 4.76 lb,
Temperature 500 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength at Break 35.0 MPa
5080 psi
5 mm/min; ISO 527
40.0 MPa
5800 psi
Type I, 5 mm/min; ASTM D638
Tensile Strength, Yield 50.0 MPa
7250 psi
Type I, 5 mm/min; ASTM D638
55.0 MPa
7980 psi
5 mm/min; ISO 527
Elongation at Break 26 %
26 %
Type I, 5 mm/min; ASTM D638
30 %
30 %
5 mm/min; ISO 527
Elongation at Yield 3.3 %
3.3 %
Type I, 5 mm/min; ASTM D638
3.8 %
3.8 %
5 mm/min; ISO 527
Tensile Modulus 4.40 GPa
638 ksi
5 mm/min; ASTM D638
4.50 GPa
653 ksi
1 mm/min; ISO 527
Flexural Yield Strength 97.0 MPa
14100 psi
1.3 mm/min, 50 mm span; ASTM D790
97.0 MPa
14100 psi
2 mm/min; ISO 178
Flexural Modulus 4.30 GPa
624 ksi
1.3 mm/min, 50 mm span; ASTM D790
4.40 GPa
638 ksi
2 mm/min; ISO 178
Izod Impact, Notched 0.600 J/cm
1.12 ft-lb/in
ASTM D256
Izod Impact, Notched (ISO) 5.00 kJ/m²
2.38 ft-lb/in²
80*10*3; ISO 180/1A
Charpy Impact, Notched 0.500 J/cm²
2.38 ft-lb/in²
Edgew 80*10*3 sp=62mm; ISO 179/1eA
Dart Drop, Total Energy 56.0 J

@Temperature 23.0 °C
41.3 ft-lb

@Temperature 73.4 °F
ASTM D3763
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 42.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
23.3 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
62.0 µm/m-°C

@Temperature 23.0 - 80.0 °C
34.4 µin/in-°F

@Temperature 73.4 - 176 °F
ISO 11359-2
CTE, linear, Transverse to Flow 49.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
27.2 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
78.0 µm/m-°C

@Temperature 23.0 - 80.0 °C
43.3 µin/in-°F

@Temperature 73.4 - 176 °F
ISO 11359-2
Deflection Temperature at 0.46 MPa (66 psi) 91.0 °C

@Thickness 3.20 mm
196 °F

@Thickness 0.126 in
unannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 85.0 °C
185 °F
Flatw 80*10*4 sp=64mm; ISO 75/Af
82.0 °C

@Thickness 3.20 mm
180 °F

@Thickness 0.126 in
unannealed; ASTM D648
Flammability, UL94 V-0

@Thickness 1.20 mm
V-0

@Thickness 0.0472 in
UL 94
Copyright © lookpolymers.com All Rights Reserved