Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

SABIC Innovative Plastics Cycoloy® RCM6134 PC+ABS (Asia Pacific)

Category Polymer , Thermoplastic , ABS Polymer , Polycarbonate/ABS Alloy, Unreinforced , Polycarbonate (PC)
Manufacturer SABIC Innovative Plastics (GE Plastics)
Trade Name Cycoloy®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF SABIC Innovative Plastics Cycoloy® RCM6134 PC+ABS (Asia Pacific).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Cycoloy* RCM6134 resin is an injection moldable filled PC/ABS blend with non-brominated and non-chlorinated flame retardant. It contains 35% post consumer recycle content with a UL-94 V0 rating @ 1.0mm. Developed for thin wall applications that require high flow and high stiffness performance. Limited availability and restricted color only.
Physical Properties Metric English Comments
Specific Gravity 1.22 g/cc
1.22 g/cc
ASTM D792
Linear Mold Shrinkage, Flow 0.0030 - 0.0050 cm/cm

@Thickness 3.20 mm
0.0030 - 0.0050 in/in

@Thickness 0.126 in
SABIC Method
Linear Mold Shrinkage, Transverse 0.0030 - 0.0050 cm/cm

@Thickness 3.20 mm
0.0030 - 0.0050 in/in

@Thickness 0.126 in
SABIC Method
Melt Flow 11 g/10 min

@Load 2.16 kg,
Temperature 260 °C
11 g/10 min

@Load 4.76 lb,
Temperature 500 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength at Break 44.0 MPa
6380 psi
Type I, 5 mm/min; ASTM D638
48.0 MPa
6960 psi
5 mm/min; ISO 527
Tensile Strength, Yield 54.0 MPa
7830 psi
Type I, 5 mm/min; ASTM D638
56.0 MPa
8120 psi
5 mm/min; ISO 527
Elongation at Break 70 %
70 %
Type I, 5 mm/min; ASTM D638
75 %
75 %
5 mm/min; ISO 527
Elongation at Yield 3.4 %
3.4 %
5 mm/min; ISO 527
3.5 %
3.5 %
Type I, 5 mm/min; ASTM D638
Tensile Modulus 3.10 GPa
450 ksi
5 mm/min; ASTM D638
3.10 GPa
450 ksi
1 mm/min; ISO 527
Flexural Yield Strength 90.0 MPa
13100 psi
1.3 mm/min, 50 mm span; ASTM D790
95.0 MPa
13800 psi
2 mm/min; ISO 178
Flexural Modulus 3.10 GPa
450 ksi
1.3 mm/min, 50 mm span; ASTM D790
3.10 GPa
450 ksi
2 mm/min; ISO 178
Izod Impact, Notched 3.00 J/cm
5.62 ft-lb/in
ASTM D256
Izod Impact, Notched (ISO) 20.0 kJ/m²
9.52 ft-lb/in²
80*10*3; ISO 180/1A
Charpy Impact, Notched 1.10 J/cm²
5.23 ft-lb/in²
Edgew 80*10*4 sp=62mm; ISO 179/1eA
Dart Drop, Total Energy 52.0 J

@Temperature 23.0 °C
38.4 ft-lb

@Temperature 73.4 °F
ASTM D3763
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 70.0 µm/m-°C

@Temperature 23.0 - 80.0 °C
38.9 µin/in-°F

@Temperature 73.4 - 176 °F
ISO 11359-2
CTE, linear, Transverse to Flow 80.0 µm/m-°C

@Temperature 23.0 - 80.0 °C
44.4 µin/in-°F

@Temperature 73.4 - 176 °F
ISO 11359-2
Deflection Temperature at 0.46 MPa (66 psi) 88.0 °C

@Thickness 3.20 mm
190 °F

@Thickness 0.126 in
unannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 81.0 °C
178 °F
Flatw 80*10*4 sp=64mm; ISO 75/Af
80.0 °C

@Thickness 3.20 mm
176 °F

@Thickness 0.126 in
unannealed; ASTM D648
Flammability, UL94 V-1

@Thickness 0.800 mm
V-1

@Thickness 0.0315 in
UL 94
V-0

@Thickness 1.00 mm
V-0

@Thickness 0.0394 in
UL 94
Users viewing this material also viewed the following: