SABIC Innovative Plastics GELOY CR7500 ASA (Europe-Africa-Middle East)

Category Polymer , Thermoplastic , ASA Polymer
Manufacturer SABIC Innovative Plastics (GE Plastics)
Trade Name GELOY
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF SABIC Innovative Plastics GELOY CR7500 ASA (Europe-Africa-Middle East).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
High heat ASA with optimum flow-impact balance. For Automotive applications and Automotive colors only.
Physical Properties Metric English Comments
Specific Gravity 1.08 g/cc
1.08 g/cc
ASTM D792
Density 1.07 g/cc
0.0387 lb/in³
ISO 1183
Moisture Absorption 0.200 %
0.200 %
23°C / 50% RH; ISO 62
Water Absorption at Saturation 0.50 %
0.50 %
ISO 62
Linear Mold Shrinkage, Flow 0.0050 - 0.0080 cm/cm

@Thickness 3.20 mm
0.0050 - 0.0080 in/in

@Thickness 0.126 in
SABIC Method
Melt Flow 6.3 g/10 min

@Load 10.0 kg,
Temperature 220 °C
6.3 g/10 min

@Load 22.0 lb,
Temperature 428 °F
ASTM D1238
11 g/10 min

@Load 5.00 kg,
Temperature 260 °C
11 g/10 min

@Load 11.0 lb,
Temperature 500 °F
ASTM D1238
Melt Index of Compound 6.0 g/10 min

@Load 10.0 kg,
Temperature 220 °C
6.0 g/10 min

@Load 22.0 lb,
Temperature 428 °F
MVR [cm^3/10 min]; ISO 1133
10 g/10 min

@Load 5.00 kg,
Temperature 260 °C
10 g/10 min

@Load 11.0 lb,
Temperature 500 °F
MVR [cm^3/10 min]; ISO 1133
Mechanical Properties Metric English Comments
Tensile Strength at Break 33.0 MPa
4790 psi
Type I, 5 mm/min; ASTM D638
35.0 MPa
5080 psi
5 mm/min; ISO 527
Tensile Strength, Yield 40.0 MPa
5800 psi
Type I, 5 mm/min; ASTM D638
43.0 MPa
6240 psi
5 mm/min; ISO 527
Elongation at Break 19 %
19 %
5 mm/min; ISO 527
60 %
60 %
Type I, 5 mm/min; ASTM D638
Elongation at Yield 3.3 %
3.3 %
5 mm/min; ISO 527
3.6 %
3.6 %
Type I, 5 mm/min; ASTM D638
Tensile Modulus 1.97 GPa
286 ksi
5 mm/min; ASTM D638
2.04 GPa
296 ksi
1 mm/min; ISO 527
Flexural Yield Strength 64.0 MPa
9280 psi
2 mm/min; ISO 178
68.0 MPa
9860 psi
1.3 mm/min, 50 mm span; ASTM D790
Flexural Modulus 2.06 GPa
299 ksi
2 mm/min; ISO 178
2.17 GPa
315 ksi
1.3 mm/min, 50 mm span; ASTM D790
Izod Impact, Notched 4.00 J/cm
7.49 ft-lb/in
ASTM D256
0.600 J/cm

@Temperature -30.0 °C
1.12 ft-lb/in

@Temperature -22.0 °F
ASTM D256
Izod Impact, Notched (ISO) 15.0 kJ/m²
7.14 ft-lb/in²
80*10*4; ISO 180/1A
6.00 kJ/m²

@Temperature -30.0 °C
2.86 ft-lb/in²

@Temperature -22.0 °F
80*10*4; ISO 180/1A
Charpy Impact, Notched 1.40 J/cm²
6.66 ft-lb/in²
Edgew 80*10*4 sp=62mm; ISO 179/1eA
Dart Drop, Total Energy 30.0 J

@Temperature 23.0 °C
22.1 ft-lb

@Temperature 73.4 °F
ASTM D3763
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 84.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
46.7 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
84.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
46.7 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
CTE, linear, Transverse to Flow 95.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
52.8 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
95.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
52.8 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
Hot Ball Pressure Test <= 98.0 °C
<= 208 °F
IEC 60695-10-2
Deflection Temperature at 1.8 MPa (264 psi) 88.0 °C
190 °F
Edgew 120*10*4 sp=100mm; ISO 75/Ae
89.0 °C
192 °F
Flatw 80*10*4 sp=64mm; ISO 75/Af
90.0 °C

@Thickness 3.20 mm
194 °F

@Thickness 0.126 in
unannealed; ASTM D648
Vicat Softening Point 98.0 °C
208 °F
Rate B/50; ASTM D1525
102 °C
216 °F
Rate B/50; ISO 306
105 °C
221 °F
Rate B/120; ISO 306