Category Polymer , Thermoplastic , ASA Polymer , Acrylonitrile/Styrene/Acrylate (ASA), Unreinforced, Molded
Manufacturer SABIC Innovative Plastics (GE Plastics)
Trade Name GELOY
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF SABIC Innovative Plastics Geloy FXTW30CP ASA.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Pearlescent GELOY ASA resin with copper-look for capstock extrusion. Outstanding weatherability.This data was supplied by SABIC-IP for the Americas region.
Physical Properties Metric English Comments
Specific Gravity 1.14 g/cc
1.14 g/cc
ASTM D 792
Density 1.12 g/cc
0.0405 lb/in³
ISO 1183
Linear Mold Shrinkage, Flow 0.00 - 0.0010 cm/cm

@Thickness 3.20 mm
0.00 - 0.0010 in/in

@Thickness 0.126 in
SABIC Method
Melt Flow 0.60 g/10 min

@Load 3.80 kg,
Temperature 200 °C
0.60 g/10 min

@Load 8.38 lb,
Temperature 392 °F
ASTM D 1238
Mechanical Properties Metric English Comments
Tensile Strength at Break 39.0 MPa
5660 psi
Type I, 5 mm/min; ASTM D 638
48.0 MPa
6960 psi
5 mm/min; ISO 527
Tensile Strength, Yield 50.0 MPa
7250 psi
Type I, 5 mm/min; ASTM D 638
50.0 MPa
7250 psi
5 mm/min; ISO 527
Elongation at Break 14 %
14 %
Type I, 5 mm/min; ASTM D 638
29 %
29 %
5 mm/min; ISO 527
Elongation at Yield 3.3 %
3.3 %
Type I, 5 mm/min; ASTM D 638
3.6 %
3.6 %
5 mm/min; ISO 527
Tensile Modulus 2.67 GPa
387 ksi
5 mm/min; ASTM D 638
2.75 GPa
399 ksi
1 mm/min; ISO 527
Flexural Yield Strength 76.0 MPa
11000 psi
2 mm/min; ISO 178
77.0 MPa
11200 psi
1.3 mm/min, 50 mm span; ASTM D 790
Flexural Modulus 2.75 GPa
399 ksi
1.3 mm/min, 50 mm span; ASTM D 790
2.78 GPa
403 ksi
2 mm/min; ISO 178
Izod Impact, Notched 0.340 J/cm

@Temperature -30.0 °C
0.637 ft-lb/in

@Temperature -22.0 °F
ASTM D 256
0.670 J/cm

@Temperature 23.0 °C
1.26 ft-lb/in

@Temperature 73.4 °F
ASTM D 256
Izod Impact, Notched (ISO) 3.00 kJ/m²

@Temperature -30.0 °C
1.43 ft-lb/in²

@Temperature -22.0 °F
80*10*4; ISO 180/1A
6.00 kJ/m²

@Temperature 23.0 °C
2.86 ft-lb/in²

@Temperature 73.4 °F
80*10*4; ISO 180/1A
Impact Test 4.00 J

@Temperature 23.0 °C
2.95 ft-lb

@Temperature 73.4 °F
Instrumented Impact Total Energy; ASTM D 3763
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 95.4 µm/m-°C

@Temperature -40.0 - 40.0 °C
53.0 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
CTE, linear, Transverse to Flow 108 µm/m-°C

@Temperature -40.0 - 40.0 °C
60.0 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
Deflection Temperature at 1.8 MPa (264 psi) 78.0 °C
172 °F
Flatw 80*10*4 sp=64mm; ISO 75/Af
76.0 °C

@Thickness 3.20 mm
169 °F

@Thickness 0.126 in
unannealed; ASTM D 648
Vicat Softening Point 86.0 °C
187 °F
Rate B/50; ISO 306
89.0 °C
192 °F
Rate B/50; ASTM D 1525