Category Polymer , Thermoplastic , Polysulfone (PSU)
Manufacturer SABIC Innovative Plastics (GE Plastics)
Trade Name LNP Colorcomp
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF SABIC Innovative Plastics LNP COLORCOMP G1000 PSU (Europe-Africa-Middle East).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
LNP* COLORCOMP* G1000-GY4A805-0 is a compound based on Polysulfone resin. Added features include: Custom Color Grey.
Physical Properties Metric English Comments
Density 1.24 g/cc
0.0448 lb/in³
ISO 1183
Water Absorption 0.40 %

@Time 86400 sec
0.40 %

@Time 24.0 hour
ISO 62-1
Linear Mold Shrinkage, Flow 0.0040 - 0.0070 cm/cm
0.0040 - 0.0070 in/in
SABIC Method
Mechanical Properties Metric English Comments
Tensile Strength at Break 60.0 MPa
8700 psi
50 mm/min; ISO 527
Tensile Strength, Yield 76.0 MPa
11000 psi
50 mm/min; ISO 527
Elongation at Yield 5.9 %
5.9 %
50 mm/min; ISO 527
Tensile Modulus 2.50 GPa
363 ksi
1 mm/min; ISO 527
Flexural Yield Strength 115 MPa
16700 psi
2 mm/min; ISO 178
Flexural Modulus 2.50 GPa
363 ksi
2 mm/min; ISO 178
Izod Impact, Notched (ISO) 6.00 kJ/m²
2.86 ft-lb/in²
80*10*4; ISO 180/1A
Izod Impact, Unnotched (ISO) NB
NB
80*10*4; ISO 180/1U
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 61.0 µm/m-°C

@Temperature 23.0 - 60.0 °C
33.9 µin/in-°F

@Temperature 73.4 - 140 °F
ISO 11359-2
CTE, linear, Transverse to Flow 62.0 µm/m-°C

@Temperature 23.0 - 60.0 °C
34.4 µin/in-°F

@Temperature 73.4 - 140 °F
ISO 11359-2
Deflection Temperature at 0.46 MPa (66 psi) 183 °C
361 °F
Flatw 80*10*4 sp=64mm; ISO 75/Bf
Deflection Temperature at 1.8 MPa (264 psi) 170 °C
338 °F
Flatw 80*10*4 sp=64mm; ISO 75/Af
Users viewing this material also viewed the following:
Copyright © lookpolymers.com All Rights Reserved