SABIC Innovative Plastics LNP FARADEX DS0036IR PC (Europe-Africa-Middle East)

Category Polymer , Thermoplastic , Polycarbonate (PC)
Manufacturer SABIC Innovative Plastics (GE Plastics)
Trade Name LNP FARADEX
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF SABIC Innovative Plastics LNP FARADEX DS0036IR PC (Europe-Africa-Middle East).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
LNP* FARADEX* DS0036IR is a compound based on Polycarbonate resin containing Stainless Steel Fiber, Flame Retardant. Added features include: Improved Paintability, Non-Brominated & Non-Chlorinated Flame Retardant, EMI/RFI- Shielding, High Impact
Physical Properties Metric English Comments
Density 1.29 g/cc
0.0466 lb/in³
ISO 1183
Linear Mold Shrinkage, Flow 0.0040 - 0.0070 cm/cm
0.0040 - 0.0070 in/in
SABIC Method
Mechanical Properties Metric English Comments
Tensile Strength, Yield 59.0 MPa
8560 psi
5 mm/min; ISO 527
Elongation at Yield 4.2 %
4.2 %
5 mm/min; ISO 527
Tensile Modulus 2.30 GPa
334 ksi
1 mm/min; ISO 527
Flexural Yield Strength 86.0 MPa
12500 psi
2 mm/min; ISO 178
Flexural Modulus 2.70 GPa
392 ksi
2 mm/min; ISO 178
Izod Impact, Notched (ISO) 14.0 kJ/m²
6.66 ft-lb/in²
80*10*4; ISO 180/1A
Izod Impact, Unnotched (ISO) 70.0 kJ/m²
33.3 ft-lb/in²
80*10*4; ISO 180/1U
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 135 °C
275 °F
Flatw 80*10*4 sp=64mm; ISO 75/Bf
Deflection Temperature at 1.8 MPa (264 psi) 124 °C
255 °F
Flatw 80*10*4 sp=64mm; ISO 75/Af
Flammability, UL94 V-2

@Thickness 1.50 - 1.65 mm
V-2

@Thickness 0.0591 - 0.0650 in
UL 94
Electrical Properties Metric English Comments
Shielding Effectiveness 40 - 55 dB

@Thickness 3.00 mm
40 - 55 dB

@Thickness 0.118 in
SABIC Method