Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

SABIC Innovative Plastics LNP Faradex NS0039XP PC+ABS (Europe-Africa-Middle East)

Category Polymer , Thermoplastic , ABS Polymer , Polycarbonate/ABS Alloy, Unreinforced , Polycarbonate (PC)
Manufacturer SABIC Innovative Plastics (GE Plastics)
Trade Name LNP FARADEX
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF SABIC Innovative Plastics LNP Faradex NS0039XP PC+ABS (Europe-Africa-Middle East).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
LNP* FARADEX* NS0039XP is a compound based on PC/ABS resin containing Stainless Steel Fiber, Flame Retardant. Added features include: Electrically Conductive, EMI/RFI Shielding, Flame retardant.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region.
Physical Properties Metric English Comments
Density 1.38 g/cc
0.0499 lb/in³
ISO 1183
Water Absorption 0.11 %

@Temperature 23.0 °C,
Time 86400 sec
0.11 %

@Temperature 73.4 °F,
Time 24.0 hour
ISO 62-1
Linear Mold Shrinkage, Flow 0.0030 - 0.0050 cm/cm
0.0030 - 0.0050 in/in
SABIC Method
Mechanical Properties Metric English Comments
Tensile Strength at Break 65.0 MPa
9430 psi
5 mm/min; ISO 527
Tensile Strength, Yield 67.0 MPa
9720 psi
5 mm/min; ISO 527
Elongation at Break 3.0 %
3.0 %
5 mm/min; ISO 527
Tensile Modulus 3.60 GPa
522 ksi
1 mm/min; ISO 527
Flexural Strength 91.0 MPa
13200 psi
2 mm/min; ISO 178
Flexural Yield Strength 110 MPa
16000 psi
2 mm/min; ISO 178
Flexural Modulus 3.20 GPa
464 ksi
2 mm/min; ISO 178
Izod Impact, Notched (ISO) 6.00 kJ/m²

@Temperature 23.0 °C
2.86 ft-lb/in²

@Temperature 73.4 °F
80*10*4; ISO 180/1A
Izod Impact, Unnotched (ISO) 25.0 kJ/m²

@Temperature 23.0 °C
11.9 ft-lb/in²

@Temperature 73.4 °F
80*10*4; ISO 180/1U
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 65.0 µm/m-°C

@Temperature 23.0 - 60.0 °C
36.1 µin/in-°F

@Temperature 73.4 - 140 °F
ISO 11359-2
CTE, linear, Transverse to Flow 73.0 µm/m-°C

@Temperature 23.0 - 60.0 °C
40.6 µin/in-°F

@Temperature 73.4 - 140 °F
ISO 11359-2
Deflection Temperature at 0.46 MPa (66 psi) 111 °C
232 °F
Flatw 80*10*4 sp=64mm; ISO 75/Bf
Deflection Temperature at 1.8 MPa (264 psi) 101 °C
214 °F
Flatw 80*10*4 sp=64mm; ISO 75/Af
Flammability, UL94 HB

@Thickness 0.800 mm
HB

@Thickness 0.0315 in
UL 94
V-1

@Thickness 1.00 mm
V-1

@Thickness 0.0394 in
UL 94
V-0

@Thickness 3.00 mm
V-0

@Thickness 0.118 in
UL 94
Electrical Properties Metric English Comments
Shielding Effectiveness 50 - 65 dB

@Thickness 3.00 mm
50 - 65 dB

@Thickness 0.118 in
SABIC Method