SABIC Innovative Plastics LNP KONDUIT OTF2AXXP PPS (Asia Pacific)

Category Polymer , Thermoplastic , Polyphenylene Sulfide (PPS)
Manufacturer SABIC Innovative Plastics (GE Plastics)
Trade Name LNP Konduit
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF SABIC Innovative Plastics LNP KONDUIT OTF2AXXP PPS (Asia Pacific).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
LNP* Konduit* OTF2AXXP is a compound based on Polyphenylene Sulfide resin containing Glass Fiber, Thermal Carbon Fiber. Added features of this material include: Thermally Conductive, Electrically Conductive.
Physical Properties Metric English Comments
Density 1.74 g/cc
0.0629 lb/in³
ASTM D792
1.74 g/cc
0.0629 lb/in³
ISO 1183
Linear Mold Shrinkage, Flow 0.0020 cm/cm

@Time 86400 sec
0.0020 in/in

@Time 24.0 hour
ASTM D955
0.0020 cm/cm

@Time 86400 sec
0.0020 in/in

@Time 24.0 hour
ISO 294
Linear Mold Shrinkage, Transverse 0.0047 cm/cm

@Time 86400 sec
0.0047 in/in

@Time 24.0 hour
ISO 294
Mechanical Properties Metric English Comments
Tensile Strength at Break 109 MPa
15800 psi
ISO 527
143 MPa
20700 psi
ASTM D638
Elongation at Break 0.20 %
0.20 %
ISO 527
0.80 %
0.80 %
ASTM D638
Tensile Modulus 51.83 GPa
7517 ksi
1 mm/min; ISO 527
Flexural Strength 199 MPa
28900 psi
ASTM D790
Flexural Modulus 41.36 GPa
5999 ksi
ASTM D790
Izod Impact, Notched 0.320 J/cm
0.599 ft-lb/in
ASTM D256
Izod Impact, Unnotched 2.72 J/cm
5.10 ft-lb/in
ASTM D4812
Izod Impact, Notched (ISO) 3.00 kJ/m²
1.43 ft-lb/in²
80*10*4; ISO 180/1A
Izod Impact, Unnotched (ISO) 11.0 kJ/m²
5.23 ft-lb/in²
80*10*4; ISO 180/1U
Dart Drop, Total Energy 3.00 J
2.21 ft-lb
Instrumented Impact Energy @ peak; ASTM D3763
Impact Test 3.00 J
2.21 ft-lb
Multiaxial Impact; ISO 6603
Coefficient of Friction, Dynamic 0.25
0.25
ASTM D3702 Modified
Coefficient of Friction, Static 0.34
0.34
ASTM D3702 Modified
K (wear) Factor 8.06 x 10-8 mm³/N-M
4.00 x 10-10 in³-min/ft-lb-hr
Washer; ASTM D3702 Modified
Thermal Properties Metric English Comments
Thermal Conductivity 2.20 W/m-K
15.3 BTU-in/hr-ft²-°F
ASTM E 1530
Deflection Temperature at 1.8 MPa (264 psi) 272 °C

@Thickness 3.20 mm
522 °F

@Thickness 0.126 in
unannealed; ASTM D648
Flammability, UL94 V-0

@Thickness 1.50 mm
V-0

@Thickness 0.0591 in
UL 94 by SABIC-IP
Electrical Properties Metric English Comments
Surface Resistance 100 ohm
100 ohm
ASTM D257