Material Notes:
LNP KONDUIT* OTF2B is a compound based on PPS - Linear resin containing 10% Glass Fiber, 55% Proprietary Thermal Filler. Added features of this material include: Thermally Conductive.
Physical Properties Metric English Comments
Density 2.20 g/cc
0.0795 lb/in³
ISO 1183
2.208 g/cc
0.07977 lb/in³
ASTM D792
Linear Mold Shrinkage, Flow 0.0045 cm/cm

@Time 86400 sec
0.0045 in/in

@Time 24.0 hour
ISO 294
0.0050 cm/cm

@Time 86400 sec
0.0050 in/in

@Time 24.0 hour
ASTM D955
Linear Mold Shrinkage, Transverse 0.0070 cm/cm

@Time 86400 sec
0.0070 in/in

@Time 24.0 hour
ASTM D955
0.0071 cm/cm

@Time 86400 sec
0.0071 in/in

@Time 24.0 hour
ISO 294
Mechanical Properties Metric English Comments
Tensile Strength at Break 83.0 MPa
12000 psi
ASTM D638
84.0 MPa
12200 psi
ISO 527
Elongation at Break 0.80 %
0.80 %
ISO 527
0.90 %
0.90 %
ASTM D638
Tensile Modulus 16.25 GPa
2357 ksi
1 mm/min; ISO 527
16.37 GPa
2374 ksi
50 mm/min; ASTM D638
Flexural Strength 136 MPa
19700 psi
ASTM D790
137 MPa
19900 psi
ISO 178
Flexural Modulus 14.85 GPa
2154 ksi
ISO 178
15.61 GPa
2264 ksi
ASTM D790
Izod Impact, Notched 0.160 J/cm
0.300 ft-lb/in
ASTM D256
Izod Impact, Unnotched 1.70 J/cm
3.18 ft-lb/in
ASTM D4812
Izod Impact, Notched (ISO) 4.00 kJ/m²
1.90 ft-lb/in²
80*10*4; ISO 180/1A
Izod Impact, Unnotched (ISO) 14.0 kJ/m²
6.66 ft-lb/in²
80*10*4; ISO 180/1U
Coefficient of Friction, Dynamic 0.51
0.51
ASTM D3702 Modified
Coefficient of Friction, Static 0.52
0.52
ASTM D3702 Modified
K (wear) Factor 8342 x 10-8 mm³/N-M
4141 x 10-10 in³-min/ft-lb-hr
Washer; ASTM D3702 Modified
Thermal Properties Metric English Comments
Thermal Conductivity 1.05 W/m-K
7.29 BTU-in/hr-ft²-°F
ASTM E 1530
Deflection Temperature at 0.46 MPa (66 psi) 264 °C
507 °F
Flatw 80*10*4 sp=64mm; ISO 75/Bf
Deflection Temperature at 1.8 MPa (264 psi) 202 °C
396 °F
Flatw 80*10*4 sp=64mm; ISO 75/Af
Flammability, UL94 V-0

@Thickness 1.50 mm
V-0

@Thickness 0.0591 in
UL 94