Material Notes:
LNP* Lubricomp* 5CL24 is a compound based on Polyvinylidene Fluoride resin containing 10% PTFE and 20% Carbon Fiber. Added features of this material include: Internally Lubricated.
Physical Properties Metric English Comments
Density 1.78 g/cc
0.0643 lb/in³
ASTM D792
Mechanical Properties Metric English Comments
Tensile Strength at Break 117 MPa
17000 psi
ASTM D638
Elongation at Break 1.3 %
1.3 %
ASTM D638
Tensile Modulus 17.07 GPa
2476 ksi
50 mm/min; ASTM D638
Flexural Strength 172 MPa
24900 psi
ASTM D790
Flexural Modulus 14.82 GPa
2149 ksi
ASTM D790