SABIC Innovative Plastics LNP LUBRICOMP BX03658N SAN

Category Polymer , Thermoplastic , SAN Polymer
Manufacturer SABIC Innovative Plastics (GE Plastics)
Trade Name LNP LUBRICOMP
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF SABIC Innovative Plastics LNP LUBRICOMP BX03658N SAN.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
LNP* LUBRICOMP* BX03658N is a compound based on SAN resin containing proprietary fillers. Added features of this grade include: Wear Resistant, Tight Dimensional Tolerances, good for Water Meter Applications.
Physical Properties Metric English Comments
Specific Gravity 1.37 g/cc
1.37 g/cc
ASTM D792
Density 1.37 g/cc
0.0495 lb/in³
ASTM D792
Moisture Absorption 0.110 %
0.110 %
50% RH, 24 hrs; ASTM D570
0.160 %
0.160 %
23°C / 50% RH; ISO 62
Linear Mold Shrinkage, Flow 0.0030 - 0.0050 cm/cm

@Time 86400 sec
0.0030 - 0.0050 in/in

@Time 24.0 hour
ASTM D955
Linear Mold Shrinkage, Transverse 0.0040 - 0.0060 cm/cm

@Time 86400 sec
0.0040 - 0.0060 in/in

@Time 24.0 hour
ASTM D955
Mechanical Properties Metric English Comments
Tensile Strength at Break 50.0 MPa
7250 psi
5 mm/min; ISO 527
52.0 MPa
7540 psi
Type I, 5 mm/min; ASTM D638
Elongation at Break 1.5 %
1.5 %
5 mm/min; ISO 527
1.5 %
1.5 %
Type I, 5 mm/min; ASTM D638
Tensile Modulus 6.13 GPa
889 ksi
1 mm/min; ISO 527
6.52 GPa
946 ksi
5 mm/min; ASTM D638
Flexural Strength 80.0 MPa
11600 psi
ISO 178
84.0 MPa
12200 psi
1.3 mm/min, 50 mm span; ASTM D790
Flexural Modulus 6.06 GPa
879 ksi
2 mm/min; ISO 178
6.32 GPa
917 ksi
1.3 mm/min, 50 mm span; ASTM D790
Izod Impact, Notched 0.170 J/cm
0.318 ft-lb/in
ASTM D256
Izod Impact, Unnotched 1.24 J/cm
2.32 ft-lb/in
ASTM D4812
Izod Impact, Notched (ISO) 2.00 kJ/m²
0.952 ft-lb/in²
80*10*4; ISO 180/1A
Izod Impact, Unnotched (ISO) 8.00 kJ/m²
3.81 ft-lb/in²
80*10*4; ISO 180/1U
Dart Drop, Total Energy 2.00 J

@Temperature 23.0 °C
1.48 ft-lb

@Temperature 73.4 °F
ASTM D3763
Coefficient of Friction, Dynamic 0.36
0.36
ASTM D3702 Modified
Coefficient of Friction, Static 0.44
0.44
ASTM D3702 Modified
K (wear) Factor 22.2 x 10-8 mm³/N-M
11.0 x 10-10 in³-min/ft-lb-hr
Ring; ASTM D3702 Modified
328 x 10-8 mm³/N-M
163 x 10-10 in³-min/ft-lb-hr
Washer; ASTM D3702 Modified
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 46.0 µm/m-°C

@Temperature -30.0 - 30.0 °C
25.6 µin/in-°F

@Temperature -22.0 - 86.0 °F
ASTM D696
CTE, linear, Transverse to Flow 53.0 µm/m-°C

@Temperature -30.0 - 30.0 °C
29.4 µin/in-°F

@Temperature -22.0 - 86.0 °F
ASTM D696
Deflection Temperature at 0.46 MPa (66 psi) 101 °C
214 °F
Flatw 80*10*4 sp=64mm; ISO 75/Bf
101 °C

@Thickness 3.20 mm
214 °F

@Thickness 0.126 in
unannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 96.0 °C
205 °F
Flatw 80*10*4 sp=64mm; ISO 75/Af
95.0 °C

@Thickness 3.20 mm
203 °F

@Thickness 0.126 in
unannealed; ASTM D648