Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

SABIC Innovative Plastics LNP LUBRICOMP DFL349EF PC

Category Polymer , Thermoplastic , Polycarbonate (PC)
Manufacturer SABIC Innovative Plastics (GE Plastics)
Trade Name LNP LUBRICOMP
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF SABIC Innovative Plastics LNP LUBRICOMP DFL349EF PC.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
LNP LUBRICOMP* DFL349EF is a compound based on Polycarbonate resin containing 20% Glass Fiber, 15% PTFE. Added features of this material include: Flame Retardant, Internally Lubricated.
Physical Properties Metric English Comments
Density 1.50 g/cc
0.0542 lb/in³
ASTM D792
1.50 g/cc
0.0542 lb/in³
ISO 1183
Moisture Absorption 0.120 %
0.120 %
23°C / 50% RH; ISO 62
Linear Mold Shrinkage, Flow 0.0040 - 0.0060 cm/cm

@Time 86400 sec
0.0040 - 0.0060 in/in

@Time 24.0 hour
ASTM D955
0.0040 - 0.0060 cm/cm

@Time 86400 sec
0.0040 - 0.0060 in/in

@Time 24.0 hour
ISO 294
Linear Mold Shrinkage, Transverse 0.0040 - 0.0060 cm/cm

@Time 86400 sec
0.0040 - 0.0060 in/in

@Time 24.0 hour
ASTM D955
0.0040 - 0.0060 cm/cm

@Time 86400 sec
0.0040 - 0.0060 in/in

@Time 24.0 hour
ISO 294
Mechanical Properties Metric English Comments
Tensile Strength at Break 88.0 MPa
12800 psi
ASTM D638
98.0 MPa
14200 psi
ISO 527
Elongation at Break 2.4 %
2.4 %
ASTM D638
3.4 %
3.4 %
ISO 527
Tensile Modulus 6.52 GPa
946 ksi
50 mm/min; ASTM D638
7.22 GPa
1050 ksi
1 mm/min; ISO 527
Flexural Strength 146 MPa
21200 psi
ISO 178
151 MPa
21900 psi
ASTM D790
Flexural Modulus 5.83 GPa
846 ksi
ISO 178
5.87 GPa
851 ksi
ASTM D790
Izod Impact, Notched 1.06 J/cm
1.99 ft-lb/in
ASTM D256
Izod Impact, Unnotched 5.01 J/cm
9.39 ft-lb/in
ASTM D4812
Izod Impact, Notched (ISO) 11.0 kJ/m²
5.23 ft-lb/in²
80*10*4; ISO 180/1A
Izod Impact, Unnotched (ISO) 40.0 kJ/m²
19.0 ft-lb/in²
80*10*4; ISO 180/1U
Dart Drop, Total Energy 15.0 J
11.1 ft-lb
Instrumented Impact Energy @ peak; ASTM D3763
Impact Test 12.0 J
8.85 ft-lb
Multiaxial Impact; ISO 6603
Coefficient of Friction, Dynamic 0.42
0.42
ASTM D3702 Modified
Coefficient of Friction, Static 0.34
0.34
ASTM D3702 Modified
K (wear) Factor 232 x 10-8 mm³/N-M
115 x 10-10 in³-min/ft-lb-hr
Washer; ASTM D3702 Modified
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 19.8 µm/m-°C

@Temperature -40.0 - 40.0 °C
11.0 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
20.2 µm/m-°C

@Temperature -40.0 - 40.0 °C
11.2 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
CTE, linear, Transverse to Flow 61.2 µm/m-°C

@Temperature -40.0 - 40.0 °C
34.0 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
61.8 µm/m-°C

@Temperature -40.0 - 40.0 °C
34.3 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
Deflection Temperature at 1.8 MPa (264 psi) 138 °C
280 °F
Flatw 80*10*4 sp=64mm; ISO 75/Af
137 °C

@Thickness 3.20 mm
279 °F

@Thickness 0.126 in
unannealed; ASTM D648
Copyright © lookpolymers.com All Rights Reserved