Material Notes:
LNP* Lubricomp* ECL36 is a compound based on Polyetherimide resin containing 30% Carbon Fiber, 15% PTFE. Added features of this material include: Internally Lubricated.
Physical Properties Metric English Comments
Density 1.48 g/cc
0.0535 lb/in³
ASTM D792
1.50 g/cc
0.0542 lb/in³
ISO 1183
Linear Mold Shrinkage, Flow 0.00040 cm/cm

@Time 86400 sec
0.00040 in/in

@Time 24.0 hour
ASTM D955
Linear Mold Shrinkage, Transverse 0.0040 cm/cm

@Time 86400 sec
0.0040 in/in

@Time 24.0 hour
ASTM D955
Mechanical Properties Metric English Comments
Tensile Strength at Break 160 MPa
23200 psi
ISO 527
179 MPa
26000 psi
ASTM D638
Elongation at Break 1.2 %
1.2 %
ISO 527
1.7 %
1.7 %
ASTM D638
Tensile Modulus 21.6 GPa
3130 ksi
1 mm/min; ISO 527
Flexural Strength 210 MPa
30500 psi
ISO 178
230 MPa
33400 psi
ASTM D790
Flexural Modulus 16.0 GPa
2320 ksi
ISO 178
19.16 GPa
2779 ksi
ASTM D790
Izod Impact, Notched 0.420 J/cm
0.787 ft-lb/in
ASTM D256
Izod Impact, Unnotched 2.67 J/cm
5.00 ft-lb/in
ASTM D4812
Izod Impact, Notched (ISO) 5.00 kJ/m²
2.38 ft-lb/in²
80*10*4; ISO 180/1A
Izod Impact, Unnotched (ISO) 18.0 kJ/m²
8.57 ft-lb/in²
80*10*4; ISO 180/1U
Coefficient of Friction, Dynamic 0.39
0.39
ASTM D3702 Modified
Coefficient of Friction, Static 0.48
0.48
ASTM D3702 Modified
K (wear) Factor 62.4 x 10-8 mm³/N-M
31.0 x 10-10 in³-min/ft-lb-hr
Washer; ASTM D3702 Modified
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 208 °C

@Thickness 3.20 mm
406 °F

@Thickness 0.126 in
unannealed; ASTM D648
Electrical Properties Metric English Comments
Surface Resistance 10 - 1.00e+6 ohm
10 - 1.00e+6 ohm
ASTM D257