Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

SABIC Innovative Plastics LNP LUBRICOMP EX00548C PEI

Category Polymer , Thermoplastic , Polyetherimide (PEI)
Manufacturer SABIC Innovative Plastics (GE Plastics)
Trade Name LNP LUBRICOMP
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF SABIC Innovative Plastics LNP LUBRICOMP EX00548C PEI.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
LNP LUBRICOMP* EX00548C is a compound based on Polyetherimide resin containing Proprietary Fillers. Added features of this material include: Clean Compounding System, Wear Resistant.
Physical Properties Metric English Comments
Density 1.31 g/cc
0.0473 lb/in³
ASTM D792
1.31 g/cc
0.0473 lb/in³
ISO 1183
Moisture Absorption 0.220 %
0.220 %
50% RH, 24 hrs; ASTM D570
Linear Mold Shrinkage, Flow 0.0066 cm/cm

@Time 86400 sec
0.0066 in/in

@Time 24.0 hour
ISO 294
0.0070 cm/cm

@Time 86400 sec
0.0070 in/in

@Time 24.0 hour
ASTM D955
Linear Mold Shrinkage, Transverse 0.0070 cm/cm

@Time 86400 sec
0.0070 in/in

@Time 24.0 hour
ASTM D955
0.0070 cm/cm

@Time 86400 sec
0.0070 in/in

@Time 24.0 hour
ISO 294
Mechanical Properties Metric English Comments
Tensile Strength at Break 83.0 MPa
12000 psi
ASTM D638
85.0 MPa
12300 psi
ISO 527
Tensile Strength, Yield 85.0 MPa
12300 psi
ASTM D638
86.0 MPa
12500 psi
ISO 527
Elongation at Break 7.6 %
7.6 %
ISO 527
8.1 %
8.1 %
ASTM D638
Elongation at Yield 6.0 %
6.0 %
ISO 527
6.1 %
6.1 %
ASTM D638
Tensile Modulus 3.03 GPa
439 ksi
50 mm/min; ASTM D638
3.20 GPa
464 ksi
1 mm/min; ISO 527
Flexural Strength 143 MPa
20700 psi
ISO 178
148 MPa
21500 psi
ASTM D790
Flexural Modulus 3.39 GPa
492 ksi
ISO 178
3.44 GPa
499 ksi
ASTM D790
Izod Impact, Notched 0.260 J/cm
0.487 ft-lb/in
ASTM D256
Izod Impact, Unnotched 4.69 J/cm
8.79 ft-lb/in
ASTM D4812
Izod Impact, Notched (ISO) 4.00 kJ/m²
1.90 ft-lb/in²
80*10*4; ISO 180/1A
Izod Impact, Unnotched (ISO) 32.0 kJ/m²
15.2 ft-lb/in²
80*10*4; ISO 180/1U
Dart Drop, Total Energy 4.00 J
2.95 ft-lb
Instrumented Impact Energy @ peak; ASTM D3763
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 184 °C
363 °F
Flatw 80*10*4 sp=64mm; ISO 75/Af
185 °C

@Thickness 3.20 mm
365 °F

@Thickness 0.126 in
unannealed; ASTM D648
Users viewing this material also viewed the following: