SABIC Innovative Plastics LNP LUBRICOMP FX04491H PE

Category Polymer , Thermoplastic , Polyethylene (PE)
Manufacturer SABIC Innovative Plastics (GE Plastics)
Trade Name LNP LUBRICOMP
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF SABIC Innovative Plastics LNP LUBRICOMP FX04491H PE.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
LNP LUBRICOMP* FX04491H is a compound based on Polyethylene resin containing Proprietary Fillers. Added features of this material include: Wear Resistant.
Physical Properties Metric English Comments
Density 0.932 g/cc
0.0337 lb/in³
ASTM D792
Linear Mold Shrinkage, Flow 0.024 cm/cm

@Time 86400 sec
0.024 in/in

@Time 24.0 hour
ASTM D955
Linear Mold Shrinkage, Transverse 0.016 cm/cm

@Time 86400 sec
0.016 in/in

@Time 24.0 hour
ASTM D955
Mechanical Properties Metric English Comments
Tensile Strength, Yield 24.0 MPa
3480 psi
ASTM D638
Elongation at Yield 7.4 %
7.4 %
ASTM D638
Flexural Strength 23.0 MPa
3340 psi
ASTM D790
Flexural Modulus 10.68 GPa
1549 ksi
ASTM D790
Izod Impact, Notched 0.450 J/cm
0.843 ft-lb/in
ASTM D256
Izod Impact, Unnotched NB
NB
ASTM D4812
Coefficient of Friction, Dynamic 0.13
0.13
ASTM D3702 Modified
Coefficient of Friction, Static 0.11
0.11
ASTM D3702 Modified
K (wear) Factor 48.3 x 10-8 mm³/N-M
24.0 x 10-10 in³-min/ft-lb-hr
Washer; ASTM D3702 Modified
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 42.0 °C

@Thickness 3.20 mm
108 °F

@Thickness 0.126 in
unannealed; ASTM D648