SABIC Innovative Plastics LNP LUBRICOMP IFL21 PA 6/12 (Asia Pacific)

Category Polymer , Thermoplastic , Nylon , Nylon 612
Manufacturer SABIC Innovative Plastics (GE Plastics)
Trade Name LNP LUBRICOMP
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF SABIC Innovative Plastics LNP LUBRICOMP IFL21 PA 6/12 (Asia Pacific).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
LNP* LUBRICOMP* IFL21 is a compound based on Nylon 6/12 resin containing PTFE, Glass Fiber. Added features of this material include: Internally Lubricated.
Physical Properties Metric English Comments
Density 1.17 g/cc
0.0423 lb/in³
ASTM D792
Mechanical Properties Metric English Comments
Tensile Strength at Break 70.0 MPa
10200 psi
ASTM D638
Elongation at Break 2.8 %
2.8 %
ASTM D638
Tensile Modulus 3.62 GPa
525 ksi
50 mm/min; ASTM D638
Flexural Strength 110 MPa
16000 psi
ASTM D790
Flexural Modulus 3.33 GPa
483 ksi
ASTM D790
Izod Impact, Notched 0.320 J/cm
0.599 ft-lb/in
ASTM D256
Izod Impact, Unnotched 2.67 J/cm
5.00 ft-lb/in
ASTM D4812
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 189 °C

@Thickness 3.20 mm
372 °F

@Thickness 0.126 in
unannealed; ASTM D648