SABIC Innovative Plastics LNP LUBRICOMP JFL24 PES (Europe-Africa-Middle East)

Category Polymer , Thermoplastic , Polyethersulfone (PES)
Manufacturer SABIC Innovative Plastics (GE Plastics)
Trade Name LNP LUBRICOMP
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF SABIC Innovative Plastics LNP LUBRICOMP JFL24 PES (Europe-Africa-Middle East).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
LNP* Lubricomp* JFL24 is a compound based on Polyethersulfone resin containing Glass Fiber, PTFE.
Physical Properties Metric English Comments
Density 1.57 g/cc
0.0567 lb/in³
ISO 1183
Mechanical Properties Metric English Comments
Tensile Strength at Break 94.0 MPa
13600 psi
5 mm/min; ISO 527
Elongation at Break 1.0 %
1.0 %
5 mm/min; ISO 527
Flexural Strength 140 MPa
20300 psi
2 mm/min; ISO 178
Flexural Modulus 5.50 GPa
798 ksi
2 mm/min; ISO 178
Izod Impact, Notched (ISO) 10.0 kJ/m²
4.76 ft-lb/in²
80*10*4; ISO 180/1A
Izod Impact, Unnotched (ISO) 30.0 kJ/m²
14.3 ft-lb/in²
80*10*4; ISO 180/1U
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 27.0 µm/m-°C

@Temperature 23.0 - 60.0 °C
15.0 µin/in-°F

@Temperature 73.4 - 140 °F
ISO 11359-2
CTE, linear, Transverse to Flow 51.0 µm/m-°C

@Temperature 23.0 - 60.0 °C
28.3 µin/in-°F

@Temperature 73.4 - 140 °F
ISO 11359-2
Deflection Temperature at 0.46 MPa (66 psi) 218 °C
424 °F
Flatw 80*10*4 sp=64mm; ISO 75/Bf
Deflection Temperature at 1.8 MPa (264 psi) 211 °C
412 °F
Flatw 80*10*4 sp=64mm; ISO 75/Af