Material Notes:
LNP* LUBRICOMP* RAL229 is a compound based on Nylon 66 containing 10% Aramid, 10% PTFE. Added features of this grade include: Flame Retardant, Wear Resistant.
Physical Properties Metric English Comments
Specific Gravity 1.42 g/cc
1.42 g/cc
ASTM D792
Mechanical Properties Metric English Comments
Tensile Strength at Break 81.0 MPa
11700 psi
Type I, 5 mm/min; ASTM D638
Elongation at Break 4.0 %
4.0 %
Type I, 5 mm/min; ASTM D638
Flexural Strength 114 MPa
16500 psi
1.3 mm/min, 50 mm span; ASTM D790
Flexural Modulus 3.72 GPa
540 ksi
1.3 mm/min, 50 mm span; ASTM D790
Izod Impact, Notched 0.370 J/cm
0.693 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 162 °C

@Thickness 3.20 mm
324 °F

@Thickness 0.126 in
unannealed; ASTM D648
Flammability, UL94 V-0

@Thickness 3.00 mm
V-0

@Thickness 0.118 in
UL 94