Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

SABIC Innovative Plastics LNP LUBRICOMP RFL25ES PA 66 (Europe-Africa-Middle East)

Category Polymer , Thermoplastic , Nylon , Nylon 66
Manufacturer SABIC Innovative Plastics (GE Plastics)
Trade Name LNP LUBRICOMP
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF SABIC Innovative Plastics LNP LUBRICOMP RFL25ES PA 66 (Europe-Africa-Middle East).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
LNP* Lubricomp* RFL25ES is a compound based on Nylon 66 resin containing Glass Fiber, PTFE. Added features of this material include: Easy Molding.
Physical Properties Metric English Comments
Density 1.40 g/cc
0.0506 lb/in³
ISO 1183
Mechanical Properties Metric English Comments
Tensile Strength at Break 145 MPa
21000 psi
5 mm/min; ISO 527
Elongation at Break 3.0 %
3.0 %
5 mm/min; ISO 527
Tensile Modulus 7.80 GPa
1130 ksi
1 mm/min; ISO 527
Flexural Strength 215 MPa
31200 psi
2 mm/min; ISO 178
Flexural Modulus 7.20 GPa
1040 ksi
2 mm/min; ISO 178
Izod Impact, Notched (ISO) 8.00 kJ/m²
3.81 ft-lb/in²
80*10*4; ISO 180/1A
7.00 kJ/m²

@Temperature -30.0 °C
3.33 ft-lb/in²

@Temperature -22.0 °F
80*10*4; ISO 180/1A
Izod Impact, Unnotched (ISO) 50.0 kJ/m²
23.8 ft-lb/in²
80*10*4; ISO 180/1U
45.0 kJ/m²

@Temperature -30.0 °C
21.4 ft-lb/in²

@Temperature -22.0 °F
80*10*4; ISO 180/1U
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 222 °C
432 °F
Flatw 80*10*4 sp=64mm; ISO 75/Af
Copyright © lookpolymers.com All Rights Reserved