Material Notes:
LNP LUBRICOMP* RFL26 is a compound based on Nylon 66 resin containing 30% Glass Fiber, 10% PTFE. Added features of this material include: Wear Resistant.
Physical Properties Metric English Comments
Density 1.46 g/cc
0.0527 lb/in³
ASTM D792
Mechanical Properties Metric English Comments
Tensile Strength at Break 185 MPa
26800 psi
ASTM D638
Elongation at Break 3.3 %
3.3 %
ASTM D638
Flexural Strength 262 MPa
38000 psi
ISO 178
275 MPa
39900 psi
ASTM D790
Impact Test 4.00 J
2.95 ft-lb
Multiaxial Impact; ISO 6603
Coefficient of Friction, Dynamic 0.61
0.61
ASTM D3702 Modified
K (wear) Factor 12.1 x 10-8 mm³/N-M
6.00 x 10-10 in³-min/ft-lb-hr
Washer; ASTM D3702 Modified
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 30.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
16.7 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831