SABIC Innovative Plastics LNP LUBRICOMP UAL23AS PPA (Europe-Africa-Middle East)

Category Polymer , Thermoplastic , Polyphthalamide (PPA)
Manufacturer SABIC Innovative Plastics (GE Plastics)
Trade Name LNP LUBRICOMP
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF SABIC Innovative Plastics LNP LUBRICOMP UAL23AS PPA (Europe-Africa-Middle East).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
LNP* LUBRICOMP* UAL23AS is a compound based on Polyphthalamide resin containing Aramide Fiber, PTFE. Added features include : Internally Lubricated, Heat Stabilized.
Physical Properties Metric English Comments
Density 1.28 g/cc
0.0462 lb/in³
ISO 1183
Mechanical Properties Metric English Comments
Tensile Strength at Break 78.0 MPa
11300 psi
5 mm/min; ISO 527
Elongation at Break 2.3 %
2.3 %
5 mm/min; ISO 527
Tensile Modulus 4.10 GPa
595 ksi
1 mm/min; ISO 527
Flexural Yield Strength 130 MPa
18900 psi
2 mm/min; ISO 178
Flexural Modulus 3.80 GPa
551 ksi
2 mm/min; ISO 178
Izod Impact, Notched (ISO) 3.00 kJ/m²
1.43 ft-lb/in²
80*10*4; ISO 180/1A
Izod Impact, Unnotched (ISO) 20.0 kJ/m²
9.52 ft-lb/in²
80*10*4; ISO 180/1U
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 235 °C
455 °F
Flatw 80*10*4 sp=64mm; ISO 75/Bf
Deflection Temperature at 1.8 MPa (264 psi) 125 °C
257 °F
Flatw 80*10*4 sp=64mm; ISO 75/Af