Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

SABIC Innovative Plastics LNP LUBRICOMP WFL34H PBT (Asia Pacific)

Category Polymer , Thermoplastic , Polyester, TP , Polybutylene Terephthalate (PBT)
Manufacturer SABIC Innovative Plastics (GE Plastics)
Trade Name LNP LUBRICOMP
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF SABIC Innovative Plastics LNP LUBRICOMP WFL34H PBT (Asia Pacific).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
LNP* LUBRICOMP* WFL34H is a compound based on Polybutylene Terephalate resin containing PTFE, Glass Fiber. Added features of this material include: Internally Lubricated.
Physical Properties Metric English Comments
Density 1.56 g/cc
0.0564 lb/in³
ASTM D792
Mechanical Properties Metric English Comments
Tensile Strength at Break 115 MPa
16700 psi
ASTM D638
Elongation at Break 2.8 %
2.8 %
ASTM D638
Tensile Modulus 7.94 GPa
1150 ksi
50 mm/min; ASTM D638
Flexural Strength 165 MPa
23900 psi
ASTM D790
Flexural Modulus 7.42 GPa
1080 ksi
ASTM D790
Izod Impact, Notched 0.850 J/cm
1.59 ft-lb/in
ASTM D256
Izod Impact, Unnotched 7.42 J/cm
13.9 ft-lb/in
ASTM D4812
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 214 °C

@Thickness 3.20 mm
417 °F

@Thickness 0.126 in
unannealed; ASTM D648
Users viewing this material also viewed the following: