Material Notes:
Wear resistant PSUThis data was supplied by SABIC-IP for the Americas region.
Physical Properties Metric English Comments
Density 1.31 g/cc
0.0473 lb/in³
ASTM D 792
Linear Mold Shrinkage, Flow 0.0051 - 0.0071 cm/cm

@Time 86400 sec
0.0051 - 0.0071 in/in

@Time 24.0 hour
ASTM D 955
Linear Mold Shrinkage, Transverse 0.0063 - 0.0083 cm/cm

@Time 86400 sec
0.0063 - 0.0083 in/in

@Time 24.0 hour
ASTM D 955
Mechanical Properties Metric English Comments
Tensile Strength at Break 48.0 MPa
6960 psi
5 mm/min; ISO 527
Tensile Strength, Yield 68.0 MPa
9860 psi
5 mm/min; ISO 527
Elongation at Break 9.3 %
9.3 %
5 mm/min; ISO 527
Elongation at Yield 5.8 %
5.8 %
5 mm/min; ISO 527
Tensile Modulus 2.52 GPa
365 ksi
1 mm/min; ISO 527
Flexural Yield Strength 88.0 MPa
12800 psi
2 mm/min; ISO 178
Flexural Modulus 2.64 GPa
383 ksi
2 mm/min; ISO 178
Izod Impact, Notched (ISO) 9.00 kJ/m²

@Temperature 23.0 °C
4.28 ft-lb/in²

@Temperature 73.4 °F
80*10*4; ISO 180/1A
Izod Impact, Unnotched (ISO) 219 kJ/m²

@Temperature 23.0 °C
104 ft-lb/in²

@Temperature 73.4 °F
80*10*4; ISO 180/1U
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 167 °C
333 °F
Flatw 80*10*4 sp=64mm; ISO 75/Af