Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

SABIC Innovative Plastics LNP Lubricomp GZL34E PSU

Category Polymer , Thermoplastic , Polysulfone (PSU)
Manufacturer SABIC Innovative Plastics (GE Plastics)
Trade Name LNP LUBRICOMP
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF SABIC Innovative Plastics LNP Lubricomp GZL34E PSU.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
LNP LUBRICOMP* GZL34E is a compound based on Polysulfone resin containing Glass Fiber, Milled Glass, PTFE. Added features of this material include: Easy Molding.This data was supplied by SABIC-IP for the Americas region.
Physical Properties Metric English Comments
Density 1.53 g/cc
0.0553 lb/in³
ASTM D 792
Linear Mold Shrinkage, Flow 0.0070 cm/cm

@Time 86400 sec
0.0070 in/in

@Time 24.0 hour
ASTM D 955
Linear Mold Shrinkage, Transverse 0.0060 cm/cm

@Time 86400 sec
0.0060 in/in

@Time 24.0 hour
ASTM D 955
Mechanical Properties Metric English Comments
Tensile Strength at Break 44.0 MPa
6380 psi
ASTM D 638
Elongation at Break 2.4 %
2.4 %
ASTM D 638
Flexural Strength 78.0 MPa
11300 psi
ASTM D 790
Flexural Modulus 3.44 GPa
499 ksi
ASTM D 790
Izod Impact, Notched 0.530 J/cm

@Temperature 23.0 °C
0.993 ft-lb/in

@Temperature 73.4 °F
ASTM D 256
Izod Impact, Unnotched 2.40 J/cm

@Temperature 23.0 °C
4.50 ft-lb/in

@Temperature 73.4 °F
ASTM D 4812