Material Notes:
LNP* Lubricomp ZI001 is a compound based on Modified PPO containing Silicone. Characteristics are internally lubricated.This data was supplied by SABIC-IP for the Americas region.
Physical Properties Metric English Comments
Specific Gravity 1.05 g/cc
1.05 g/cc
ASTM D 792
Density 1.05 g/cc
0.0379 lb/in³
ASTM D 792
Moisture Absorption at Equilibrium 0.10 %
0.10 %
23°C / 50% RH; ISO 62
0.090 %

@Time 86400 sec
0.090 %

@Time 24.0 hour
50% RH; ASTM D 570
Linear Mold Shrinkage, Flow 0.0070 - 0.0090 cm/cm

@Time 86400 sec
0.0070 - 0.0090 in/in

@Time 24.0 hour
ASTM D 955
Linear Mold Shrinkage, Transverse 0.0090 - 0.011 cm/cm

@Time 86400 sec
0.0090 - 0.011 in/in

@Time 24.0 hour
ASTM D 955
Mechanical Properties Metric English Comments
Tensile Strength at Break 47.0 MPa
6820 psi
5 mm/min; ISO 527
51.0 MPa
7400 psi
Type I, 5 mm/min; ASTM D 638
Tensile Strength, Yield 37.0 MPa
5370 psi
5 mm/min; ISO 527
44.0 MPa
6380 psi
Type I, 5 mm/min; ASTM D 638
Elongation at Break 35.7 %
35.7 %
Type I, 5 mm/min; ASTM D 638
44.7 %
44.7 %
5 mm/min; ISO 527
Elongation at Yield 2.3 %
2.3 %
5 mm/min; ISO 527
2.7 %
2.7 %
Type I, 5 mm/min; ASTM D 638
Tensile Modulus 2.40 GPa
348 ksi
1 mm/min; ISO 527
2.50 GPa
363 ksi
50 mm/min; ASTM D 638
Flexural Strength 72.0 MPa
10400 psi
ISO 178
Flexural Modulus 2.38 GPa
345 ksi
2 mm/min; ISO 178
2.52 GPa
365 ksi
1.3 mm/min, 50 mm span; ASTM D 790
Izod Impact, Notched 1.55 J/cm

@Temperature 23.0 °C
2.90 ft-lb/in

@Temperature 73.4 °F
ASTM D 256
Izod Impact, Unnotched 15.7 J/cm

@Temperature 23.0 °C
29.4 ft-lb/in

@Temperature 73.4 °F
ASTM D 4812
Izod Impact, Notched (ISO) 14.0 kJ/m²

@Temperature 23.0 °C
6.66 ft-lb/in²

@Temperature 73.4 °F
80*10*4; ISO 180/1A
Izod Impact, Unnotched (ISO) 135 kJ/m²

@Temperature 23.0 °C
64.2 ft-lb/in²

@Temperature 73.4 °F
80*10*4; ISO 180/1U
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 118 °C
244 °F
Flatw 80*10*4 sp=64mm; ISO 75/Af
117 °C

@Thickness 3.20 mm
243 °F

@Thickness 0.126 in
unannealed; ASTM D 648