Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

SABIC Innovative Plastics LNP STAT-KON 9X06519 Cyclic Olefinic Copolymer

Category Polymer , Thermoplastic , Cyclo Olefin Polymer
Manufacturer SABIC Innovative Plastics (GE Plastics)
Trade Name LNP STAT-KON
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF SABIC Innovative Plastics LNP STAT-KON 9X06519 Cyclic Olefinic Copolymer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
LNP STAT-KON* 9X06519 is a compound based on Cyclic Olefinic Copolymer resin containing 30% Carbon Fiber. Added features of this material include: Clean Compounding System, Electrically Conductive.
Physical Properties Metric English Comments
Density 1.17 g/cc
0.0423 lb/in³
ASTM D792
Mechanical Properties Metric English Comments
Tensile Strength at Break 74.0 MPa
10700 psi
ASTM D638
Elongation at Break 0.50 %
0.50 %
ASTM D638
Tensile Modulus 16.04 GPa
2326 ksi
50 mm/min; ASTM D638
Flexural Strength 158 MPa
22900 psi
ASTM D790
Flexural Modulus 16.68 GPa
2419 ksi
ASTM D790
Izod Impact, Notched 0.320 J/cm
0.599 ft-lb/in
ASTM D256
Izod Impact, Unnotched 1.22 J/cm
2.29 ft-lb/in
ASTM D4812
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 2.80 µm/m-°C

@Temperature -40.0 - 40.0 °C
1.56 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
CTE, linear, Transverse to Flow 12.6 µm/m-°C

@Temperature -40.0 - 40.0 °C
7.00 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
Deflection Temperature at 1.8 MPa (264 psi) 150 °C

@Thickness 3.20 mm
302 °F

@Thickness 0.126 in
unannealed; ASTM D648
Electrical Properties Metric English Comments
Surface Resistance 10 ohm - 1e+05
10 ohm - 1e+05
ASTM D257