SABIC Innovative Plastics LNP STAT-KON AX02747 ABS (Asia Pacific)

Category Polymer , Thermoplastic , ABS Polymer
Manufacturer SABIC Innovative Plastics (GE Plastics)
Trade Name LNP STAT-KON
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF SABIC Innovative Plastics LNP STAT-KON AX02747 ABS (Asia Pacific).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
LNP* Stat-kon* AX02747 is a compound based on Acrylonitrile Butadiene Styrene resin containing Proprietary Filler(s). Added features of this material include: Electrically Conductive.
Physical Properties Metric English Comments
Density 1.24 g/cc
0.0448 lb/in³
ASTM D792
Mechanical Properties Metric English Comments
Tensile Strength at Break 106 MPa
15400 psi
ASTM D638
Elongation at Break 1.0 %
1.0 %
ASTM D638
Tensile Modulus 19.98 GPa
2898 ksi
50 mm/min; ASTM D638
Flexural Strength 179 MPa
26000 psi
ASTM D790
Flexural Modulus 18.09 GPa
2624 ksi
ASTM D790
Izod Impact, Notched 0.420 J/cm
0.787 ft-lb/in
ASTM D256
Electrical Properties Metric English Comments
Surface Resistance 10 - 1000 ohm
10 - 1000 ohm
ASTM D257