Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

SABIC Innovative Plastics LNP STAT-KON DE0029EF PC

Category Polymer , Thermoplastic , Polycarbonate (PC)
Manufacturer SABIC Innovative Plastics (GE Plastics)
Trade Name LNP STAT-KON
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF SABIC Innovative Plastics LNP STAT-KON DE0029EF PC.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
LNP STAT-KON* DE0029EF is a compound based on Polycarbonate resin containing 10% Carbon Fiber. Added features of this material include: Easy Molding. Flame Retardant, Electrically Conductive.
Physical Properties Metric English Comments
Density 1.26 g/cc
0.0455 lb/in³
ASTM D792
1.26 g/cc
0.0455 lb/in³
ISO 1183
Moisture Absorption 0.160 %
0.160 %
50% RH, 24 hrs; ASTM D570
0.200 %
0.200 %
23°C / 50% RH; ISO 62
Linear Mold Shrinkage, Flow 0.00060 - 0.0032 cm/cm

@Time 86400 sec
0.00060 - 0.0032 in/in

@Time 24.0 hour
ISO 294
0.0010 - 0.0030 cm/cm

@Time 86400 sec
0.0010 - 0.0030 in/in

@Time 24.0 hour
ASTM D955
Linear Mold Shrinkage, Transverse 0.0020 - 0.0040 cm/cm

@Time 86400 sec
0.0020 - 0.0040 in/in

@Time 24.0 hour
ASTM D955
0.0029 - 0.0043 cm/cm

@Time 86400 sec
0.0029 - 0.0043 in/in

@Time 24.0 hour
ISO 294
Mechanical Properties Metric English Comments
Tensile Strength at Break 114 MPa
16500 psi
ASTM D638
117 MPa
17000 psi
ISO 527
Elongation at Break 2.3 %
2.3 %
ASTM D638
2.4 %
2.4 %
ISO 527
Tensile Modulus 8.50 GPa
1230 ksi
1 mm/min; ISO 527
8.89 GPa
1290 ksi
50 mm/min; ASTM D638
Flexural Strength 180 MPa
26100 psi
ASTM D790
183 MPa
26500 psi
ISO 178
Flexural Modulus 7.65 GPa
1110 ksi
ASTM D790
8.80 GPa
1280 ksi
ISO 178
Izod Impact, Notched 0.600 J/cm
1.12 ft-lb/in
ASTM D256
Izod Impact, Unnotched 4.44 J/cm
8.32 ft-lb/in
ASTM D4812
Izod Impact, Notched (ISO) 6.00 kJ/m²
2.86 ft-lb/in²
80*10*4; ISO 180/1A
Izod Impact, Unnotched (ISO) 29.0 kJ/m²
13.8 ft-lb/in²
80*10*4; ISO 180/1U
Dart Drop, Total Energy 17.0 J
12.5 ft-lb
Instrumented Impact Energy @ peak; ASTM D3763
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 23.5 µm/m-°C

@Temperature -40.0 - 40.0 °C
13.1 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
23.6 µm/m-°C

@Temperature -40.0 - 40.0 °C
13.1 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
CTE, linear, Transverse to Flow 34.5 µm/m-°C

@Temperature -40.0 - 40.0 °C
19.2 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
34.6 µm/m-°C

@Temperature -40.0 - 40.0 °C
19.2 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
Deflection Temperature at 0.46 MPa (66 psi) 144 °C

@Thickness 3.20 mm
291 °F

@Thickness 0.126 in
unannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 139 °C
282 °F
Flatw 80*10*4 sp=64mm; ISO 75/Af
140 °C

@Thickness 3.20 mm
284 °F

@Thickness 0.126 in
unannealed; ASTM D648
Electrical Properties Metric English Comments
Surface Resistance 100 - 1.00e+6 ohm
100 - 1.00e+6 ohm
ASTM D257
Users viewing this material also viewed the following:
Copyright © lookpolymers.com All Rights Reserved