Category Polymer , Thermoplastic , Polycarbonate (PC)
Manufacturer SABIC Innovative Plastics (GE Plastics)
Trade Name LNP STAT-KON
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF SABIC Innovative Plastics LNP STAT-KON DEL13PXC PC (Europe-Africa-Middle East).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
LNP* Stat-kon* DEL13PXC is a compound based on Polycarbonate resin containing PTFE, Carbon Fiber. Added features of this material include: Electrically Conductive, Superior Molding.
Physical Properties Metric English Comments
Density 1.29 g/cc
0.0466 lb/in³
ISO 1183
Mechanical Properties Metric English Comments
Tensile Strength at Break 142 MPa
20600 psi
5 mm/min; ISO 527
Elongation at Break 1.8 %
1.8 %
5 mm/min; ISO 527
Tensile Modulus 10.6 GPa
1540 ksi
1 mm/min; ISO 527
Flexural Yield Strength 191 MPa
27700 psi
2 mm/min; ISO 178
Flexural Modulus 9.00 GPa
1310 ksi
2 mm/min; ISO 178
Izod Impact, Notched (ISO) 8.00 kJ/m²
3.81 ft-lb/in²
80*10*4; ISO 180/1A
Izod Impact, Unnotched (ISO) 30.0 kJ/m²
14.3 ft-lb/in²
80*10*4; ISO 180/1U
Thermal Properties Metric English Comments
CTE, linear, Transverse to Flow 14.0 µm/m-°C

@Temperature 23.0 - 60.0 °C
7.78 µin/in-°F

@Temperature 73.4 - 140 °F
ISO 11359-2
Deflection Temperature at 0.46 MPa (66 psi) 139 °C
282 °F
Flatw 80*10*4 sp=64mm; ISO 75/Bf
Deflection Temperature at 1.8 MPa (264 psi) 134 °C
273 °F
Flatw 80*10*4 sp=64mm; ISO 75/Af
Electrical Properties Metric English Comments
Surface Resistance 100 - 10000 ohm
100 - 10000 ohm
ASTM D257