Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

SABIC Innovative Plastics LNP STAT-KON DEL22P PC

Category Polymer , Thermoplastic , Polycarbonate (PC)
Manufacturer SABIC Innovative Plastics (GE Plastics)
Trade Name LNP STAT-KON
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF SABIC Innovative Plastics LNP STAT-KON DEL22P PC.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
LNP STAT-KON* DEL22P is a compound based on Polycarbonate resin containing 10% Carbon Fiber, 10% PTFE. Added features of this material include: Electrically Conductive. Exceptional Processing, Wear Resistant.
Physical Properties Metric English Comments
Density 1.30 g/cc
0.0470 lb/in³
ASTM D792
1.30 g/cc
0.0470 lb/in³
ISO 1183
Moisture Absorption 0.100 %
0.100 %
50% RH, 24 hrs; ASTM D570
0.180 %
0.180 %
23°C / 50% RH; ISO 62
Linear Mold Shrinkage, Flow 0.0010 - 0.0030 cm/cm
0.0010 - 0.0030 in/in
SABIC Method
0.0010 - 0.0030 cm/cm

@Thickness 0.750 - 2.30 mm
0.0010 - 0.0030 in/in

@Thickness 0.0295 - 0.0906 in
SABIC Method
Linear Mold Shrinkage, Transverse 0.0040 - 0.0060 cm/cm
0.0040 - 0.0060 in/in
SABIC Method
0.0040 - 0.0060 cm/cm

@Thickness 0.750 - 2.30 mm
0.0040 - 0.0060 in/in

@Thickness 0.0295 - 0.0906 in
SABIC Method
Mechanical Properties Metric English Comments
Tensile Strength at Break 100 MPa
14500 psi
ASTM D638
101 MPa
14600 psi
ISO 527
Elongation at Break 2.0 %
2.0 %
ASTM D638
2.0 %
2.0 %
ISO 527
Tensile Modulus 7.90 GPa
1150 ksi
50 mm/min; ASTM D638
8.17 GPa
1180 ksi
1 mm/min; ISO 527
Flexural Strength 152 MPa
22000 psi
ASTM D790
Flexural Modulus 0.150 GPa
21.8 ksi
ISO 178
5.69 GPa
825 ksi
ASTM D790
Izod Impact, Notched 0.740 J/cm
1.39 ft-lb/in
ASTM D256
Izod Impact, Unnotched 2.83 J/cm
5.30 ft-lb/in
ASTM D4812
Izod Impact, Notched (ISO) 6.00 kJ/m²
2.86 ft-lb/in²
80*10*4; ISO 180/1A
Izod Impact, Unnotched (ISO) 34.0 kJ/m²
16.2 ft-lb/in²
80*10*4; ISO 180/1U
Dart Drop, Total Energy 13.0 J
9.59 ft-lb
Instrumented Impact Energy @ peak; ASTM D3763
Impact Test 102 J
75.2 ft-lb
Multiaxial Impact; ISO 6603
Coefficient of Friction, Dynamic 0.55
0.55
ASTM D3702 Modified
Coefficient of Friction, Static 0.52
0.52
ASTM D3702 Modified
K (wear) Factor 30.2 x 10-8 mm³/N-M
15.0 x 10-10 in³-min/ft-lb-hr
Washer; ASTM D3702 Modified
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 14.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
7.78 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
15.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
8.33 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
CTE, linear, Transverse to Flow 76.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
42.2 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
76.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
42.2 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
Deflection Temperature at 1.8 MPa (264 psi) 143 °C
289 °F
Flatw 80*10*4 sp=64mm; ISO 75/Af
134 °C

@Thickness 3.20 mm
273 °F

@Thickness 0.126 in
unannealed; ASTM D648
Electrical Properties Metric English Comments
Volume Resistivity 100 ohm-cm
100 ohm-cm
IEC 60093
Surface Resistance 100 - 1.00e+6 ohm
100 - 1.00e+6 ohm
ROA; IEC 60093
Users viewing this material also viewed the following:
Copyright © lookpolymers.com All Rights Reserved