SABIC Innovative Plastics LNP STAT-KON DEL329E PC

Category Polymer , Thermoplastic , Polycarbonate (PC)
Manufacturer SABIC Innovative Plastics (GE Plastics)
Trade Name LNP STAT-KON
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF SABIC Innovative Plastics LNP STAT-KON DEL329E PC.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
LNP* Stat-kon* DEL329E is a compound based on Polycarbonate resin containing 10% Carbon Fiber, 15% PTFE. Added features of this material include: Electrically Conductive, Flame Retardant, Wear Resistant, Easy Molding.
Physical Properties Metric English Comments
Density 1.40 g/cc
0.0506 lb/in³
ASTM D792
Mechanical Properties Metric English Comments
Tensile Strength at Break 99.0 MPa
14400 psi
ASTM D638
Elongation at Break 1.8 %
1.8 %
ASTM D638
Tensile Modulus 9.92 GPa
1440 ksi
50 mm/min; ASTM D638
Flexural Strength 158 MPa
22900 psi
ASTM D790
Flexural Modulus 8.96 GPa
1300 ksi
ASTM D790
Izod Impact, Notched 0.690 J/cm
1.29 ft-lb/in
ASTM D256
Izod Impact, Unnotched 3.73 J/cm
6.99 ft-lb/in
ASTM D4812
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 145 °C

@Thickness 3.20 mm
293 °F

@Thickness 0.126 in
unannealed; ASTM D648
Electrical Properties Metric English Comments
Surface Resistance 1.0 - 6.0 ohm
1.0 - 6.0 ohm
ASTM D257