SABIC Innovative Plastics LNP STAT-KON DEL36 PC (Europe-Africa-Middle East)

Category Polymer , Thermoplastic , Polycarbonate (PC)
Manufacturer SABIC Innovative Plastics (GE Plastics)
Trade Name LNP STAT-KON
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF SABIC Innovative Plastics LNP STAT-KON DEL36 PC (Europe-Africa-Middle East).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
LNP* STATKON* DEL36 is a compound based on Polycarbonate resin containing Carbon Fiber, PTFE. Added features include: Electrically Conductive, Internally Lubricated.
Physical Properties Metric English Comments
Density 1.43 g/cc
0.0517 lb/in³
ISO 1183
Mechanical Properties Metric English Comments
Tensile Strength at Break 169 MPa
24500 psi
5 mm/min; ISO 527
Elongation at Break 1.6 %
1.6 %
5 mm/min; ISO 527
Tensile Modulus 15.8 GPa
2290 ksi
1 mm/min; ISO 527
Flexural Yield Strength 194 MPa
28100 psi
2 mm/min; ISO 178
Flexural Modulus 13.4 GPa
1940 ksi
2 mm/min; ISO 178
Izod Impact, Notched (ISO) 9.00 kJ/m²
4.28 ft-lb/in²
80*10*4; ISO 180/1A
Izod Impact, Unnotched (ISO) 30.0 kJ/m²
14.3 ft-lb/in²
80*10*4; ISO 180/1U
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 18.0 µm/m-°C

@Temperature 23.0 - 60.0 °C
10.0 µin/in-°F

@Temperature 73.4 - 140 °F
ISO 11359-2
CTE, linear, Transverse to Flow 53.0 µm/m-°C

@Temperature 23.0 - 60.0 °C
29.4 µin/in-°F

@Temperature 73.4 - 140 °F
ISO 11359-2
Deflection Temperature at 1.8 MPa (264 psi) 135 °C
275 °F
Flatw 80*10*4 sp=64mm; ISO 75/Af
Electrical Properties Metric English Comments
Surface Resistance 10 - 1000 ohm
10 - 1000 ohm
ASTM D257