Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

SABIC Innovative Plastics LNP STAT-KON DX05301C PC (Asia Pacific)

Category Polymer , Thermoplastic , Polycarbonate (PC)
Manufacturer SABIC Innovative Plastics (GE Plastics)
Trade Name LNP STAT-KON
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF SABIC Innovative Plastics LNP STAT-KON DX05301C PC (Asia Pacific).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Low Ionic, Low Outgassing, Low LPC and ESD safe Polycarbonate compound suitable for Semiconductor and Hard Disk Drive (HDD) application.Added features of this material include: Clean Compounding System.This product is also known as STAT-KON PDX-D-05301 CCS.
Physical Properties Metric English Comments
Specific Gravity 1.22 g/cc
1.22 g/cc
ASTM D792
Density 1.22 g/cc
0.0441 lb/in³
ISO 1183
Linear Mold Shrinkage, Flow 0.0060 cm/cm
0.0060 in/in
SABIC Method
Linear Mold Shrinkage, Transverse 0.0060 cm/cm
0.0060 in/in
SABIC Method
Melt Flow 22.6 g/10 min

@Load 5.00 kg,
Temperature 300 °C
22.6 g/10 min

@Load 11.0 lb,
Temperature 572 °F
ASTM D1238
Melt Index of Compound 22 g/10 min

@Load 5.00 kg,
Temperature 300 °C
22 g/10 min

@Load 11.0 lb,
Temperature 572 °F
MVR [cm^3/10 min]; ISO 1133
Mechanical Properties Metric English Comments
Tensile Strength at Break 56.0 MPa
8120 psi
5 mm/min; ISO 527
60.0 MPa
8700 psi
Type I, 5 mm/min; ASTM D638
Tensile Strength, Yield 48.0 MPa
6960 psi
Type I, 5 mm/min; ASTM D638
56.0 MPa
8120 psi
5 mm/min; ISO 527
Elongation at Break 1.5 %
1.5 %
5 mm/min; ISO 527
9.9 %
9.9 %
Type I, 5 mm/min; ASTM D638
Elongation at Yield 1.5 %
1.5 %
5 mm/min; ISO 527
5.3 %
5.3 %
Type I, 5 mm/min; ASTM D638
Tensile Modulus 2.49 GPa
361 ksi
1 mm/min; ISO 527
2.59 GPa
376 ksi
5 mm/min; ASTM D638
Flexural Yield Strength 77.0 MPa
11200 psi
2 mm/min; ISO 178
95.0 MPa
13800 psi
1.3 mm/min, 50 mm span; ASTM D790
Flexural Modulus 2.28 GPa
331 ksi
1.3 mm/min, 50 mm span; ASTM D790
2.48 GPa
360 ksi
2 mm/min; ISO 178
Izod Impact, Notched 0.540 J/cm
1.01 ft-lb/in
ASTM D256
Izod Impact, Notched (ISO) 5.00 kJ/m²
2.38 ft-lb/in²
80*10*4; ISO 180/1A
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 131 °C
268 °F
Flatw 80*10*4 sp=64mm; ISO 75/Af
132 °C

@Thickness 3.20 mm
270 °F

@Thickness 0.126 in
unannealed; ASTM D648
Vicat Softening Point 146 °C
295 °F
Rate B/120; ISO 306
Electrical Properties Metric English Comments
Volume Resistivity 1e+05 - 1.00e+8 ohm-cm
1e+05 - 1.00e+8 ohm-cm
ASTM D257
Surface Resistance 1e+05 - 1.00e+8 ohm
1e+05 - 1.00e+8 ohm
ASTM D257
Static Decay 0.10 sec
0.10 sec
5000V to <50V; FTMS101B
Copyright © lookpolymers.com All Rights Reserved